MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Lubrizol LifeSciences Carbothane® AC-4075A TPU – Clear Aromatic
Categories: Polymer; Thermoplastic; Polyurethane, TP

Material Notes: Medical Grade Aromatic Polycarbonate-based Thermoplastic Polyurethane (TPU)

Features: good mechanical properties, good chemical resistance, excellent oxidative stability and biocompatibility properties and can be color-matched

Process: Extrusion and Injection Molding

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.19 g/cc1.19 g/ccASTM D792
Linear Mold Shrinkage 0.011 cm/cm0.011 in/in1”x.25”x6” bar; ASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 7777ASTM D785
Tensile Strength, Ultimate 55.2 MPa8000 psiASTM D412
Elongation at Break 400 %400 %ASTM D412
100% Modulus 2.76 MPa
@Strain 100 %
400 psi
@Strain 100 %
ASTM D412
200% Modulus 7.067 MPa
@Strain 200 %
1025 psi
@Strain 200 %
ASTM D412
300% Modulus 30.3 MPa
@Strain 300 %
4400 psi
@Strain 300 %
ASTM D412
Flexural Modulus 0.0103 GPa1.50 ksiASTM D790
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 91.0 °C196 °FASTM D1525
Glass Transition Temp, Tg -23.0 °C-9.40 °F
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 195 °C383 °FInjection
Front Barrel Temperature 200 °C392 °FInjection
Nozzle Temperature 195 °C383 °FInjection
Zone 1 210 °C410 °FExtrusion
Zone 2 215 °C419 °FExtrusion
Zone 3 221 °C430 °FExtrusion
Zone 4 221 °C430 °FExtrusion
Adapter Temperature 215 °C419 °FExtrusion
Die Temperature 215 °C419 °FExtrusion
Melt Temperature 200 °C392 °FInjection
Mold Temperature 10.0 - 27.0 °C50.0 - 80.6 °FInjection

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Lubrizol LifeSciences Carbothane® PC-3575A TPU – Clear Aliphatic
Huntsman IROGRAN® A 80 P 5039 TPU-Polyether
Huntsman IROGRAN® A 70 E 4675 Polyester-Based TPU-High Performance Grade
Lubrizol LifeSciences Pellethane® 2363-55DE TPU
Lubrizol LifeSciences Carbothane® PC-3555D TPU – Clear Aliphatic

PLUBR9011 / 203578

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.