MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Versalis Flexirene® FH 56 A Butene Copolymer Linear Low Density Polyethylene
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE); Linear Low Density Polyethylene (LLDPE), Film Grade; LLDPE/Butene, Film

Material Notes: Flexirene FH 56 A is a butene copolymer with medium density (C4-LLDPE), with antioxidants and processing aid, suitable for blown film extrusion.

Films manufactured with Flexirene FH 56 A are characterized by a good rigidity and an optimum processability.

Main Applications: Flexirene FH 56 A is recommended for the production of general purpose film in blend or in coextrusion with LDPE. It is also used for the production of nets because of its perfect balance between rigidity and processability.

Information provided by Polimeri Europa.

Versalis is the Eni subsidiary containing the plastics and rubber businesses.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.934 g/ccISO 1183
Thickness 15.0 - 50.0 micronsRecommended
Melt Flow 1.4 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Film Tensile Strength at Yield, MD 16.0 MPaISO 527-3
Film Tensile Strength at Yield, TD 18.0 MPaISO 527-3
Film Elongation at Break, MD 650 %ISO 527-3
Film Elongation at Break, TD 800 %ISO 527-3
Coefficient of Friction, Dynamic >= 0.50ISO 8295
Elmendorf Tear Strength, MD 0.7133 g/micronISO 6383-2
Elmendorf Tear Strength, TD 6.114 g/micronISO 6383-2
Dart Drop Test 55.0 gF50; ISO 7765-1
Film Tensile Strength at Break, MD 40.0 MPaISO 527-3
Film Tensile Strength at Break, TD 32.0 MPaISO 527-3
1% Secant Modulus, MD 390 MPaISO 527-3
1% Secant Modulus, TD 450 MPaISO 527-3
 
Thermal PropertiesOriginal ValueComments
Melting Point 126 °CInternal method
Vicat Softening Point 117 °C
@Load 1.00 kg
ISO 306/A
Brittleness Temperature <= -70.0 °CASTM D746
 
Optical PropertiesOriginal ValueComments
Haze 14 %ISO 14782
Gloss 50 %45°; ASTM D2457

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PENG095 / 124489

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.