MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

TriSteel

(Viewing data as-entered. Click here to return)
Saint-Gobain Fluoroloy® A22 High Performance Seal Material
Categories: Polymer; Thermoplastic

Material Notes: Resistant to abrasions; Proprietary custom PEEK; Chemical and environmental inertness; Good strength at elevated temperatures

Information provided by Saint-Gobain Performance Plastics.

Vendors: TriStar Plastics Corp. provides engineering, custom fabrication and manufacturing of high-performance plastics and self-lubricating bearing materials, such as Fluoroloy®, Rulon, PEEK, Torlon, CJ Composites and Ultracomp. Capabilities include component design, material selection, prototype and production, manufacturing and surface modification. Call (800) TRI-STAR (800) 874-7827 or visit or www.TStar.com

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.30 g/ccASTM D792
Deformation 0.030 %
@Time 86400 sec
13.8 MPa (2000 psi) load; ASTM D621
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 90ASTM D2240
Tensile Strength 95.0 MPaASTM D4894
Elongation at Break 30 %ASTM D4894
Tensile Modulus 4.00 GPaASTM D4894
Compressive Yield Strength 138 MPa
@Strain 1 %
ASTM D695
Compressive Modulus 2.441 GPaASTM D695
Coefficient of Friction 0.40Saint-Gobain Method
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 55.6 µm/m-°C
@Temperature 26.0 - 200 °C
Mold Direction; ASTM D696
CTE, linear, Transverse to Flow 78.5 µm/m-°C
@Temperature 26.0 - 200 °C
ASTM D696
Maximum Service Temperature, Air 260 °C
 
Descriptive Properties
ColorTan

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Saint-Gobain Fluoroloy® A08 High Performance Seal Material
Saint-Gobain Fluoroloy® A30 High Performance PTFE/Glass Seal Material
Saint-Gobain Fluoroloy® A09 High Performance Seal Material
Saint-Gobain Fluoroloy® A01 High Performance Seal Material
Saint-Gobain Fluoroloy® A12 High Performance Seal Material

PSTGQ966 / 150505

TriSteel

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.