MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Solvay GEROPON® TC 42 Surfactant
Categories: Fluid; Other Engineering Material; Additive/Filler for Polymer

Material Notes: Description: A paste form of Sodium Methyl Cocoyl Taurate that exhibits good lathering properties. Displays excellent dispersibilty properties in hard water and high electrolyte loads. Compliant with the EU's detergent biodegradability regulation.

Chemical Name: SODIUM N-COCONUT ACID-N-METHYL-TAURATE

CAS: 61791-42-2

Solubility: Soluble in water.

Available in: Asia Pacific, Europe, Latin America and North America

Applications: GEROPON® TC-42 is a coconut fatty acid derived anionic surfactant with excellent detergency and wetting properties. A mild surfactant with good foam boosting properties, GEROPON® TC-42 exhibits soap like lathering characteristics even in hard water. GEROPON® TC-42 is primarily used as a secondary foaming agent in skin cleanser and shampoo formulations.

Information provided by Rhodia, Rhodia has been acquired by Solvay.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.16 g/cc
pH 7.0 - 8.010% Solution; RP-0420
 
Chemical PropertiesOriginal ValueComments
Ionic Impurities - Fe (Iron) <= 15 ppmO-PHENANTHROLINE; RP-0277
 
Thermal PropertiesOriginal ValueComments
Melting Point 12.0 °C
 
Processing PropertiesOriginal ValueComments
Shelf Life 24.0 Month
 
Descriptive Properties
AppearanceSoft, Smooth White PasteRP-0064
CompositionActive24-26%, EQ WT. 363, RP-0027
 Free Amine<1.5, As Methyltaurine, RP-0793
 Free Fatty Acid<2.0%, EQ. WT. 218, RP-0007
 Sodium Chloride3-6%, RP-0097
Ionic ChargeAnionic
Micro Limits<10 CFU/G (No Pathogens)APC, COA

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Solvay GEROPON® T/36 DF Surfactant
Solvay GEROPON® T/36 Surfactant
Solvay GEROPON® SS OIP LPH Surfactant
Solvay GEROPON® SDS Surfactant
Solvay GEROPON® SC/213 Surfactant

WRHOD136 / 137367

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.