MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Trelleborg Fillite® SGHA (500HA) Alumino-silicate Cenospheres
Categories: Ceramic; Glass; Oxide; Silicon Oxide; Other Engineering Material; Additive/Filler for Polymer

Material Notes: Fillite is a glass hard, inert, hollow silicate sphere. Fillite is primarily used to reduce the weight of plastics, rubbers, resins, cement, etc., but also imparts further benefits in many situations. Many of the advantages from the use of Fillite, including increased filler loading and improved rheology, are directly attributed to the spherical nature of the material.

Typical Applications
SGHA has a higher alumina content than the normal Fillite grades and has been specifically developed for higher temperature applications such as refractories, foundry applications, high temperature resistant coatings. Other higher alumina grades are whiter in color and particularly suitable for gypsum board jointing compounds, veneering plasters, stuccos, sealants, coatings and cast resins.

Advantages
Reduced weight, increased filler loadings, better flow characteristics, less shrinkage and warping. Improved physical properties in moldings, castings, and laminates, reduced water absorption, improved flame retardance, improved chemical resistance.

All information provided by Fillite

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.400 - 0.480 g/cc
Pellet Density 0.700 - 0.900 g/cc
Loss On Ignition <= 2.0 %
Particle Size 5.0 - 500 µm
 
Mechanical PropertiesOriginal ValueComments
Hardness, Mohs 5.0
Compressive Strength 2000 - 4000 psiCrush Strength
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 0.110 W/m-K
Melting Point 1400 °C
 
Processing PropertiesOriginal ValueComments
Moisture Content <= 0.30 %Surface
 
Component Elements PropertiesOriginal ValueComments
Al2O3 34 - 39 %
CO2 70 %
Fe2O3 <= 2.0 %
Nitrogen, N 30 %
SiO2 55 - 65 %
 
Descriptive Properties
Average Wall Thickness (% Sphere Diameter)5-10
ColorOff-White
Packing Factor (%)60-65
Particle Size Distribution (%)100% Passing 500 microns
 10-30% Passing 100 microns
 2-10% Passing 50 microns
 30-70% Passing 150 microns
 85-100% Passing 300 microns

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
3M K20 Glass Bubbles
3M K15 Glass Bubbles
3M K1 Glass Bubbles
3M S22 Glass Bubbles
3M S15 Glass Bubbles

PTRELL202 / 83960

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.