MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

3M Scotch-Weld™ Medium Instant Wood Adhesives and Surface Activator
Categories: Polymer; Adhesive; Thermoset; Acrylic/Cyanoacrylate Adhesive

Material Notes: 3M™ Scotch-Weld™ Instant Wood Adhesives an Surface Activator are single component, room temperature-curing adhesives that provides cure and speed and shear strength for demanding applications in the manufacture and repair of furniture, cabinets, and other wood products.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Viscosity >= 450 cP>= 450 cP
 
Mechanical PropertiesMetricEnglishComments
Shear Strength 2.07 MPa300 psiOverlap, Particleboard, Substrate Failure
 2.76 MPa400 psiOverlap, Melamine, Substrate Failure
 3.10 MPa450 psiOverlap, Pine, Substrate/Cohesive Failure
 3.10 MPa450 psiOverlap, MDF, Cohesive Failure
 3.45 MPa500 psiOverlap, Polyurethane Finish, Adhesive Failure
 4.14 MPa600 psiOverlap, Polyacrylic Finish, Cohesive Failure
 6.21 MPa900 psiOverlap, Poplar, Substrate/Cohesive Failure
 6.21 MPa900 psiOverlap, High Pressure Laminate, Substrate Failure
 6.89 MPa1000 psiOverlap, Plywood, Cohesive Failure
 7.24 MPa1050 psiOverlap, Maple, Substrate Failure
 13.4 MPa1950 psiOverlap, Aluminum, Adhesive Failure
 16.2 MPa2350 psiOverlap, Oak, Substrate/Cohesive Failure
 19.7 MPa2850 psiOverlap, Steel, Adhesive Failure
 3.10 MPa
@Temperature 32.0 °C
450 psi
@Temperature 89.6 °F
Overlap, Aluminum, 90% RH, Adhesive Failure
 3.79 MPa
@Temperature 32.0 °C
550 psi
@Temperature 89.6 °F
Overlap, Polyurethane Finish, 90% RH, Adhesive Failure
 4.14 MPa
@Temperature 32.0 °C
600 psi
@Temperature 89.6 °F
Overlap, Pine, 90% RH, Adhesive Failure
 6.55 MPa
@Temperature 32.0 °C
950 psi
@Temperature 89.6 °F
Overlap, Plywood, 90% RH, Substrate Failure
 6.89 MPa
@Temperature 66.0 °C
1000 psi
@Temperature 151 °F
Overlap, Polyurethane Finish, Adhesive Failure
 7.24 MPa
@Temperature 66.0 °C
1050 psi
@Temperature 151 °F
Overlap, Plywood, Substrate Failure
 7.24 MPa
@Temperature 66.0 °C
1050 psi
@Temperature 151 °F
Overlap, Aluminum, Adhesive Failure
 7.58 MPa
@Temperature 66.0 °C
1100 psi
@Temperature 151 °F
Overlap, Pine, Adhesive Failure
 12.8 MPa
@Temperature 66.0 °C
1850 psi
@Temperature 151 °F
Overlap, Oak, Substrate/Adhesive Failure
 13.4 MPa
@Temperature 32.0 °C
1950 psi
@Temperature 89.6 °F
Overlap, Oak, 90% RH, Substrate/Adhesive Failure
 
Processing PropertiesMetricEnglishComments
Cure Time 1440 min24.0 hourFull Cure
 
Descriptive Properties
AppearanceClear-Slightly yellow liquid

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
3M Scotch-Weld™ Thin Instant Wood Adhesives and Surface Activator
Mitsubishi Chemical Advanced Materials Plastic Composites MultiQ® Concrete Thermoplastic Panel Composite
Oriented Strand Board (OSB), Aspen
Mitsubishi Chemical Advanced Materials Plastic Composites MultiQ® Impact Thermoplastic Panel Composite
3M Scotch-Weld™ Thick Instant Wood Adhesives and Surface Activator

PMM34739 / 169486

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.