- GBLT-600S is an alternative to GLT and GFLT for fuel seals and fuel injector O-rings
- Good fuel, methanol, and fluids resistance, improved vs. GLT
- Low temperature Tg, TR-10, and sealing improved vs. Viton® GFLT
- Heat resistance comparable to Viton® GLT-600S and GFLT-600S Good mold release / mold fouling properties
- Good physical properties with high elongation, both original and aged
- Good water and steam resistance / low volume swell in water
- Excellent compression set resistance with either low or no postcure F169