MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

(Viewing data as-entered. Click here to return)
Celanese FORTRON® 9140L4 40% Glass Reinforced Polyphenylene Sulfide (PPS)
Categories: Polymer; Thermoplastic; Polyphenylene Sulfide (PPS); Polyphenylene Sulfide (PPS) with 40% Glass Fiber Filler

Material Notes: Description: Fortron 9140L4 is a 40% glass fiber reinforced injection molding grade that exhibits excellent heat and chemical resistance, inherent flame retardancy, and high hardness and rigidity at elevated temperatures. Components made of this grade may be used for medical and food handling applications. Fortron 9140L4 is in compliance with ISO 10993, USP Class VI, and is included in the Fortron Drug and Device Master Files at the FDA. The grade complies with the FDA Food Contact Notification (FCN-No. 40) for repeat-use applications.

Information provided by Celanese Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.65 g/ccISO 1183
Water Absorption at Saturation 0.020 %ISO 62
Linear Mold Shrinkage 0.0020 - 0.0060 cm/cmISO 294-4
Linear Mold Shrinkage, Transverse 0.0040 - 0.0060 cm/cmISO 294-4
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 100ISO 2039-2
Tensile Strength at Break 190 MPa5 mm/min; ISO 527-2/1A
Elongation at Break 1.8 %5 mm/min; ISO 527-2/1A
Flexural Strength 280 MPaISO 178
Flexural Modulus 14.0 GPaISO 178
Izod Impact, Notched (ISO) 10.0 kJ/m²ISO 180/1A
Izod Impact, Unnotched (ISO) 32.0 kJ/m²ISO 180/1U
Charpy Impact Unnotched 4.80 J/cm²ISO 179/1eU
Charpy Impact, Notched 0.900 J/cm²ISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
Melting Point 280 °CISO 11357-1,2,3
Deflection Temperature at 1.8 MPa (264 psi) 270 °CISO 75-1, -2
Deflection Temperature at 8.0 MPa 200 °CISO 75-1, -2
Glass Transition Temp, Tg 90.0 °CISO 11357-1,-2,-3
 
Processing PropertiesOriginal ValueComments
Melt Temperature 310 - 340 °C
Mold Temperature 135 - 160 °C
Drying Temperature 275 °F
Dry Time 3 - 4 hour
 
Compliance PropertiesOriginal ValueComments
USP Class VI Yes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Celanese FORTRON 4184L4 PPS, 53% Mineral / Glass Reinforced
Celanese FORTRON 1140L6 PPS, 40% Glass Reinforced
Celanese Fortron® 1140 A0 Polyphenylene Sulfide (PPS), 40% Glass Fiber
Celanese FORTRON 1140L4 PPS, 40% Glass Reinforced
Celanese Fortron® 1140 L4 Polyphenylene Sulfide (PPS), 40% Glass Fiber

PHCW47 / 45988

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.