MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Westlake Elevate™ EF561 6.5% Ethylene Vinyl Acetate Copolymer
Categories: Polymer; Thermoplastic; Ethylene Vinyl Acetate

Material Notes: Westlake EF 561 resin is a fractional melt index 6.5% EVA copolymer designed for ice bags, frozen food bags, and other films that require excellent toughness and good heat sealing characteristics. This Kosher compliant resin has excellent low temperature brittleness properties.

    Application/Uses
  • Frozen food packaging
  • Fresh food packaging
  • Ice bags
  • Heavy duty produce bags

FDA: This material complies with FDA regulations in 21 CFR, section 177.1350. Kosher Compliant.

All information provided by Westlake Chemical

Key Words: Excellent toughness and good heat sealing characteristics. 6.5% EVA.
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Vinyl Acetate Content 6.5 %6.5 %
Thickness 31.8 microns1.25 mil
Melt Flow 0.55 g/10 min0.55 g/10 minASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Film Elongation at Break, MD 380 %380 %ASTM D882
Film Elongation at Break, TD 550 %550 %ASTM D882
Dart Drop 18.9 g/micron480 g/milASTM D1709
Film Tensile Strength at Break, MD 24.1 MPa3500 psiASTM D882
Film Tensile Strength at Break, TD 25.5 MPa3700 psiASTM D882
1% Secant Modulus, MD 103 MPa15000 psiASTM D882
1% Secant Modulus, TD 110 MPa16000 psiASTM D882
 
Optical PropertiesMetricEnglishComments
Haze 4.8 %4.8 %ASTM D1003
Gloss 74 %74 %at 45º; ASTM D2457
 
Processing PropertiesMetricEnglishComments
Melt Temperature 182 - 199 °C360 - 390 °Fwith BUR of 1.5:1 or higher
Blow-up Ratio (BUR) 2.52.5
 
Descriptive Properties
processFilm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Lushan EV1050G2 EVA Film for Encapsulating Solar modules, High Transmittance
Lushan EV1050G1 EVA Film for Encapsulating Solar modules, Ultra Fast Cure
LG Chemical SEETEC ES440 Ethylene Vinyl Acetate
LG Chemical SEETEC EF443 Ethylene Vinyl Acetate
LG Chemical SEETEC EF321 Ethylene Vinyl Acetate

PWESF8930 / 133283

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.