MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

SABIC NORYL PPX™ Resin PPX7200U Polyphenylene Ether + PP (PPE+PP) (Americas)
Categories: Polymer; Thermoplastic; Polyphenylene Ether/PPO; Polypropylene (PP)

Material Notes: NORYL PPX™ 7200U resin is a non-reinforced alloy of polyphenylene ether (PPE) + polypropylene (PP). This UV-stabilized, injection moldable grade exhibits improved chemical resistance and surface aesthetics along with high-temperature performance, excellent melt strength, modulus, impact resistance, hydrolytic and dimensional stability. NORYL PPX7200U resin is an excellent candidate for applications such as hot water tank components and outdoor housings and enclosures.

Features: Hydrolytic Stability,Chemical Resistance,Low Creep Sensitivity,Low Warpage,Aesthetics & Visual effects

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.990 g/cc0.990 g/ccASTM D792
Density 0.990 g/cc0.0358 lb/in³ISO 1183
Moisture Absorption 0.0200 %0.0200 %Injection Molding
Viscosity 18 cP
@Load 5.00 kg,
Temperature 260 °C
18 cP
@Load 11.0 lb,
Temperature 500 °F
MVR cc/10 min; ISO 1133
Linear Mold Shrinkage, Flow 0.0060 - 0.0080 cm/cm0.0060 - 0.0080 in/inSABIC method
 0.0060 - 0.0080 cm/cm
@Thickness 3.20 mm
0.0060 - 0.0080 in/in
@Thickness 0.126 in
SABIC method
Linear Mold Shrinkage, Transverse 0.0060 - 0.0080 cm/cm
@Thickness 3.20 mm
0.0060 - 0.0080 in/in
@Thickness 0.126 in
SABIC method
Melt Flow 16 g/10 min
@Load 5.00 kg,
Temperature 260 °C
16 g/10 min
@Load 11.0 lb,
Temperature 500 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 27.0 MPa3920 psi50 mm/min; ASTM D638
 28.0 MPa4060 psi50 mm/min; ISO 527
Tensile Strength, Yield 33.0 MPa4790 psi50 mm/min; ASTM D638
 34.0 MPa4930 psi50 mm/min; ISO 527
Elongation at Break 115 %115 %50 mm/min; ISO 527
 130 %130 %50 mm/min; ASTM D638
Elongation at Yield 8.2 %8.2 %50 mm/min; ISO 527
 10 %10 %50 mm/min; ASTM D638
Tensile Modulus 1.24 GPa180 ksi50 mm/min; ASTM D638
 1.67 GPa242 ksi1 mm/min; ISO 527
Flexural Strength 48.0 MPa6960 psiyld, 1.3 mm/min, 50 mm span; ASTM D790
 48.0 MPa6960 psiyield, 2 mm/min; ISO 178
Flexural Modulus 1.44 GPa209 ksi1.3 mm/min, 50 mm span; ASTM D790
 1.60 GPa232 ksi2 mm/min; ISO 178
Izod Impact Notched 149 J110 ft-lbASTM D256
Izod Impact, Unnotched 14.41 J/cm27.00 ft-lb/inASTM D4812
Izod Impact, Notched (ISO) 14.0 kJ/m²6.66 ft-lb/in²80*10*4; ISO 180/1A
 8.00 kJ/m²
@Temperature -30.0 °C
3.81 ft-lb/in²
@Temperature -22.0 °F
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) NBNB80*10*4; ISO 180/1U
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
80*10*4; ISO 180/1U
Charpy Impact Unnotched NBNBEdgew 80*10*4 sp=62mm; ISO 179/1eU
 8.00 J/cm²
@Temperature -30.0 °C
38.1 ft-lb/in²
@Temperature -22.0 °F
Edgew 80*10*4 sp=62mm; ISO 179/1eU
Charpy Impact, Notched 1.20 J/cm²5.71 ft-lb/in²Edgew 80*10*4 sp=62mm; ISO 179/1eA
 0.600 J/cm²
@Temperature -30.0 °C
2.86 ft-lb/in²
@Temperature -22.0 °F
Edgew 80*10*4 sp=62mm; ISO 179/1eA
Dart Drop, Total Energy 36.0 J26.6 ft-lbASTM D3763
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 99.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
55.0 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
CTE, linear, Transverse to Flow 108 µm/m-°C
@Temperature -40.0 - 40.0 °C
60.0 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
Deflection Temperature at 0.46 MPa (66 psi) 110 °C
@Thickness 3.20 mm
230 °F
@Thickness 0.126 in
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 71.0 °C
@Thickness 3.20 mm
160 °F
@Thickness 0.126 in
unannealed; ASTM D648
Vicat Softening Point 103 °C217 °FRate B/50; ISO 306
 107 °C225 °FRate B/120; ISO 306
 146 °C295 °FRate B/50; ASTM D1525
Flammability, UL94 HB
@Thickness >=1.50 mm
HB
@Thickness >=0.0591 in
UL 94
 
Processing PropertiesMetricEnglishComments
Nozzle Temperature 260 - 290 °C500 - 554 °F
Zone 2 240 - 280 °C464 - 536 °F
Zone 3 250 - 290 °C482 - 554 °F
Melt Temperature 260 - 290 °C500 - 554 °FInjection Molding
Mold Temperature 30.0 - 50.0 °C86.0 - 122 °F
Drying Temperature 60.0 - 65.0 °C140 - 149 °FInjection Molding
Dry Time 2.00 - 4.00 hour2.00 - 4.00 hourInjection Molding
 8.00 hour8.00 hourCumulative; Injection Molding
Back Pressure 0.300 - 0.700 MPa43.5 - 102 psi
Shot Size 30 - 70 %30 - 70 %
Vent Depth 0.00380 - 0.00510 cm0.00150 - 0.00201 in
Screw Speed 20 - 100 rpm20 - 100 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABH82226 / 290173

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.