Paroil 51-NR is a chlorinated compound. It is a nonflammable, non-corrosive, low volatile liquid at room temperature. It contains a stabilizer to maintain product integrity during transport and storage. Paroil 51-NR is used in a wide variety of applications including flame retardants, plasticizers and EP metalworking packages. For metalworking applications, Paroil 51-NR is typically (but not limited to) applied in straight oil machining, drawing and stamping fluids.Information provided by DoverChem |