MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

Permabond TA459 Toughened Acrylic Adhesive
Categories: Polymer; Adhesive; Thermoset; Acrylic/Cyanoacrylate Adhesive

Material Notes: Permabond TA459 is a structural acrylic adhesive designed primarily for bonding metals, ferrites, ceramics and some thermoplastics. This product was specifically designed to be non-corrosive to sensitive copper parts or other electrically conductive surfaces. The fast curing rate and rapid strength development of this material allows for increased production rate. Mix ratio 10:1.5 (adhesive:initiator).

Features & Benefits:

  • Adhesion to a wide variety of substrates
  • Fast cure at room temperature
  • Excellent adhesion to metals and ferrites
  • Acid-free and non-corrosive
  • No mix application
  • High shear strength
  • Good impact strength
  • Good chemical resistance

Information provided by Permabond.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.14 g/cc1.14 g/ccUncured
Viscosity 10000 - 20000 cP
@Temperature 25.0 °C
10000 - 20000 cP
@Temperature 77.0 °F
Uncured
Storage Temperature 5.00 - 25.0 °C41.0 - 77.0 °F
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 20.0 - 30.0 MPa
@Temperature 25.0 °C
2900 - 4350 psi
@Temperature 77.0 °F
stainless steel after 24 hours
Adhesive Bond Strength 4.00 MPa580 psiFerrite/steel after 3 mins, Shear
 9.00 MPa1310 psiSteel/steel after 3 mins, Shear
 >= 14.0 MPa>= 2030 psiFerrite/steel after 24 hours, Shear
 12.0 - 18.0 MPa1740 - 2610 psiZinc Plated after 24 hours, Shear
 20.0 - 25.0 MPa2900 - 3630 psiSteel/steel after 24 hours, Shear
 
Processing PropertiesMetricEnglishComments
Cure Time <= 0.250 min<= 0.00417 hourzinc, fixture time with initiator 44
 0.250 - 0.500 min0.00417 - 0.00833 hourzinc, fixture time with initiator 43
 1440 min24.0 hourfull cure
 <= 2.00 min
@Temperature 25.0 °C
<= 0.0333 hour
@Temperature 77.0 °F
with initiator 44, 50% rh
 <= 3.00 min
@Temperature 25.0 °C
<= 0.0500 hour
@Temperature 77.0 °F
with initiator 43, 50% rh
Shelf Life 12.0 Month12.0 Month
 
Descriptive Properties
AppearanceBlue, thixotropicUncured
Maximum Gap Fill (mm)0.5
Strength Retention100% at 0°CRelative to 0°C
 30% at 150°CRelative to 0°C
 5% at 200°CRelative to 0°C
 80% at 100°CRelative to 0°C
 95% at 50°CRelative to 0°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PPERMA914 / 162780

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.