MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Copper Zinc Alloy, UNS C66850, M10 Temper, Forgings
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: Temper: As Hot Forged - Air Cooled

Fabrication Properties: Excellent Suitability – Soldering, Brazing, Seam Weld; Good Suitability – Capacity for Being Hot Formed; Fair Suitability – Oxyacetylene Welding, Gas Shielded Arc Welding, Coated Metal Arc Welding, Spot Weld, Capacity for Being Cold Worked; Poor Suitability – Butt Weld

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.05 g/cc0.291 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell B 130 - 140130 - 140
Tensile Strength 480 - 520 MPa69600 - 75400 psi
 500 MPa72500 psiTypical
Elongation at Break 15 - 30 %15 - 30 %
Tensile Modulus 95.8 GPa13900 ksi
Modulus of Rigidity 35.9 GPa5200 ksi
Compressive Yield Strength >= 1230 MPa>= 178000 psi
Poissons Ratio 0.340.34
Machinability 65 %65 %
Forgeability 70 %70 %
Shear Strength 263 MPa38100 psi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000300 ohm-cm0.0000300 ohm-cm5.7% IACS
 
Thermal PropertiesMetricEnglishComments
CTE, linear  13.9 µm/m-°C
@Temperature 20.0 - 100 °C
7.73 µin/in-°F
@Temperature 68.0 - 212 °F
 19.73 µm/m-°C
@Temperature 20.0 - 200 °C
10.96 µin/in-°F
@Temperature 68.0 - 392 °F
 21.69 µm/m-°C
@Temperature 20.0 - 300 °C
12.05 µin/in-°F
@Temperature 68.0 - 572 °F
Specific Heat Capacity 0.414 J/g-°C0.0990 BTU/lb-°F
Thermal Conductivity 2.41 W/m-K16.7 BTU-in/hr-ft²-°F
Melting Point 866 - 950.0 °C1590 - 1742 °F
Solidus 866 °C1590 °F
Liquidus 950.0 °C1742 °F
Annealing Point >= 720.0 °C>= 1328 °F
 
Processing PropertiesMetricEnglishComments
Processing Temperature 300 °C572 °FStress Relief
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 0.50 - 1.5 %0.50 - 1.5 %
Copper, Cu 60 - 64 %60 - 64 %
Iron, Fe 0.50 - 1.5 %0.50 - 1.5 %
Lead, Pb <= 0.090 %<= 0.090 %
Manganese, Mn 4.0 - 8.0 %4.0 - 8.0 %
Nickel, Ni <= 0.50 %<= 0.50 %
Phosphorus, P <= 0.050 %<= 0.050 %
Tin, Sn <= 0.60 %<= 0.60 %
Zinc, Zn 25.3 - 35 %25.3 - 35 %As Balance
 
Descriptive Properties
US EPA Registered AntimicrobialYes

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

MC66850x1 / 292290

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.