MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Celanese Celanex® 3100 7.5% Fiberglass Reinforced Polybutylene Terephthalate
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), 10% Glass Fiber Filled

Material Notes: Description: Celanex 3100 is a general purpose, 7.5% glass reinforced polybutylene terephthalate with a good balance of mechanical properties and processability. Celanex 3100 is a high flow material.

Information provided by Celanese Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.35 g/ccISO 1183 & ASTM D792
Linear Mold Shrinkage 0.0060 - 0.010 cm/cmASTM D955
Melt Flow 17 g/10 minASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 78.0 MPa5 mm/min; ISO 527-2/1A
 9700 psiASTM D638
Tensile Strength, Yield 11500 psiASTM D638
Elongation at Break 8.0 %5 mm/min; ISO 527-2/1A
 8.5 %ASTM D638
Tensile Modulus 450000 psiASTM D638
Flexural Strength 105 MPaISO 178
Flexural Yield Strength 16000 psiASTM D790
Flexural Modulus 3.55 GPaISO 178
 500000 psiASTM D790
Izod Impact, Notched (ISO) 3.80 kJ/m²ISO 180/1A
Izod Impact, Unnotched (ISO) 23.0 kJ/m²ISO 180/1U
Charpy Impact Unnotched NBISO 179/1eU
 19.0 J/cm²
@Temperature -30.0 °C
ISO 179/1eU
Charpy Impact, Notched 0.600 J/cm²ISO 179/1eA
 0.550 J/cm²
@Temperature -30.0 °C
ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+13 ohm-cmIEC 60093
 1.00e+15 ohm-cmASTM D257
Surface Resistance >= 1.00e+15 ohmIEC 60093
Dielectric Constant 3.6
@Frequency 1e+6 Hz
IEC 60250
 4.0
@Frequency 100 Hz
IEC 60250
Dielectric Strength 23.0 kV/mmIEC 60243-1
 470 V/milShort Term; ASTM D149
Dissipation Factor 0.0013
@Frequency 100 Hz
IEC 60250
 0.020
@Frequency 1e+6 Hz
IEC 60250
Arc Resistance 130 secASTM D495
Comparative Tracking Index 250 VASTM D3638
 
Thermal PropertiesOriginal ValueComments
CTE, linear 130 µm/m-°C
@Temperature 20.0 °C
ISO 11359-2
Melting Point 225 °CISO 11357-1,2,3 & ASTM D3418
Deflection Temperature at 0.46 MPa (66 psi) 206 °CISO 75-1, -2
Deflection Temperature at 1.8 MPa (264 psi) 143 °CISO 75-1, -2
Flammability, UL94 HB
@Thickness 0.710 mm
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 230 - 240 °C
Middle Barrel Temperature 235 - 250 °C
Front Barrel Temperature 240 - 260 °C
Nozzle Temperature 250 - 260 °C
Melt Temperature 235 - 260 °C
Mold Temperature 65.0 - 93.0 °C
Drying Temperature 250 °F
Dry Time 4 hour
Back Pressure 0.000 - 50.0 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
BASF Ultradur® B 2550 PBT
BASF Ultradur® B 2300 G6 HR BK15116 30% Glass Filled PBT
Celanese Celanex® XFR 6842 GF15 PBT, 30% Glass Reinforced

PHCV95 / 45936

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.