MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

LCY Globalene 3501 Styrene - Butadiene block copolymer
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE); Styrene Butadiene Rubber

Material Notes: Styrene - Butadiene block copolymer specially designed for asphalt modification, compounding and for solvent based adhesive applications.

Molecular Structure: Linear
Styrene Content: 30% By weight
Butadiene Content: 70% By weight
Physical Form: Porous Pellet

Information provided by LCY Chemical Corp.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.940 g/cc0.0340 lb/in³Value; ASTM D792
Volatiles 0.17 %0.17 %Value; ASTM D5668
 <= 1.0 %<= 1.0 %Range; ASTM D5668
Brookfield Viscosity 4300 - 6200 cP4300 - 6200 cPRange; ASTM D2196
 5400 cP5400 cPValue; ASTM D2196
Ash 0.11 %0.11 %Value; ASTM D5667
 <= 1.0 %<= 1.0 %Range; ASTM D5667
 
Chemical PropertiesMetricEnglishComments
Styrene Content 32 %32 %Bound, Value
 30 - 34 %30 - 34 %Bound, Range
 
Descriptive Properties
Content>84%Coupling Efficiency, Range, ASTM D5296
 0.9Coupling Efficiency, Value, ASTM D5296

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PLCY173 / 295716

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.