MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Momentive Performance Materials GE Silicones IGS3760 High-modulus, neutral curing sealant
Categories: Polymer; Thermoset; Silicone

Material Notes: IGS3760 adhesive silicone is an optimized, high-modulus, neutral curing sealant for edge seal applications for gas and air filled structural and non-structural insulating glass units. IGS3760 two-component silicone offers variable work life to accommodate scheduling and production needs.

Features: High Modulus, High Elastic Recovery, Fast Cure, Compatibility, Non-flammable.

Applications: Structural Glazing, Silicone Durability, Adhesive. Note: IGS3760 silicone should only be used in the fabrication of insulating glass where the dual seal method of fabrication is used. The moisture vapor transmission rate of silicone sealants is sufficiently high as to preclude their use in the fabrication of single seal insulating glass units.

Information provided by Momentive Performance Materials.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.11 g/ccIGS3760B. Uncured.
 1.47 g/cc
 1.50 g/ccIGS3760A. Uncured.
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 55ASTM D2240
Tensile Strength 1.00 MPaISO 8339
 1.12 MPaASTM C1135
Tensile Strength, Ultimate 2.10 MPaASTM D412
Tensile Stress at Strain 0.440 MPa
@Strain 10 %
ASTM C1135
 0.700 MPa
@Strain 25 %
ISO 8339
 0.860 MPa
@Strain 25 %
ASTM C1135
Elongation at Break 46 %ASTM C1135
 60 %ISO 8339
Elongation, Ultimate 222 %ASTM D412
Modulus of Elasticity 2.60 GPaETAG 002
Shear Strength 0.900 MPaASTM C961
Tear Strength 6.61 kg(f)/cmDie B.; ASTM D624
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 300 °FHeat Resistance
 
Processing PropertiesOriginal ValueComments
Tack-Free Time 40.0 - 175 min
Shelf Life 12.0 MonthIGS3760B
 18.0 MonthIGS3760A
 
Descriptive Properties
Accelerated WeatheringExcellent, no degradation.5000hrs.
AppearanceThixotropic PasteIGS3760A. Uncured.
 Thixotropic PasteIGS3760B. Uncured.
ColorBlackBlack: IGS3760A mixed with IGS3760B Black
 BlackIGS3760B. Uncured.
 Black/GrayCured
 Black/GrayMixed
 Gray/whiteIGS3760A. Uncured.
Consistency / Sag<0.05”Non-sagging
Design Stress in Tension0.15 MpaETAG 002
Gas Permeability0.924 g/m2hEN1279-4
Mix Ratio12.5:1As Tested
 8:1 to 11:1Mixed by volume
Resistance to Tearingcategory 1ETAG 002.
Snap Time20-85 minutes
Water Penetration23.4 g/m2EN1279-4

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PMOMEN9923 / 265733

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.