MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

3M Dyneon™ TF 2025 PTFE  (discontinued **)
Categories: Polymer; Thermoplastic; Fluoropolymer; Polytetrafluoroethylene (PTFE)

Material Notes:
  • Processable by standard paste extrusion methods
  • Both grades can be processed at low to medium reduction ratios
  • TF 2021 PTFE is preferred for unsintered thread sealing tapes and expanded joint sealants
  • TF 2025 PTFE is recommended for pipe liner and applications because of its superior green strength

Information provided by Dyneon, A 3M Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.510 g/cc0.0184 lb/in³ASTM D4895
Density 2.15 g/cc0.0777 lb/in³ASTM D4895
Particle Size 500 µm500 µmaverage; ASTM D4895
Thickness 1600 microns63.0 mil
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 28.0 MPa4060 psiASTM D4895
Elongation at Break 340 %340 %ASTM D4895
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+19 ohm-cm1.00e+19 ohm-cmIEC 60093
Surface Resistance 1.00e+18 ohm1.00e+18 ohmIEC 60093
 
Descriptive Properties
Extrusion Pressure40 MPareduction ratio 400, ASTM D4894
Reduction Ratio Range20-300:1Dyneon Method

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PDYNE040 / 34848

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.