MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Beologic Beobase 20 ASA wood INJ047 Injection Molding
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; ASA Polymer

Material Notes: Main properties: visual wood fiber, high up resistance, high stiffness. Applications: general purpose, industrial goods, furniture, household, non-food packaging, outdoor

Information provided by Beologic.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.13 g/cc0.0408 lb/in³ISO 1183-1
Melt Flow 10.5 g/10 min
@Load 10.0 kg,
Temperature 220 °C
10.5 g/10 min
@Load 22.0 lb,
Temperature 428 °F
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 50.9 MPa7380 psiISO 527-1
Elongation at Break 2.2 %2.2 %ISO 527-1
Tensile Modulus 4.37 GPa634 ksiISO 527-1
Flexural Modulus 3.657 GPa530.4 ksiISO 178
Charpy Impact Unnotched 1.42 J/cm²6.76 ft-lb/in²ISO 179-1eU
Charpy Impact, Notched 0.300 J/cm²1.43 ft-lb/in²ISO 179-1eA
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 95.8 °C204 °FISO 75-1 (B)
Vicat Softening Point 96.1 °C205 °FB120; ISO 306
 
Descriptive Properties
Beologic Article Number2080070047
Carbon footprint (kg CO2 eq/kg)0.802PAS 2050
Renewable contentyes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PBEOL9859 / 314145

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.