MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

SunChemical Gwent D2070423D5 Polymer Dielectric
Categories: Fluid; Polymer

Material Notes: Grey colored screen printable polymer dielectric, suitable for defining electrode areas and forms a protective layer over the electrode tracking during immersion of the electrode. The formulation is designed for maximum flexibility.
Screen Printing Equipment: semi-automatic, automatic
Screen Types: stainless steel, polyester, mesh 156-325tpi
Substrate: Polyester, PVC, Polycarbonate, Ceramic or Alumina.

Information provided by Gwent Electronic Materials Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Solids Content 43 - 45 %
@Temperature 150 °C
43 - 45 %
@Temperature 302 °F
Viscosity 14000 - 16000 cP
@Shear Rate 230 1/s,
Temperature 25.0 °C
14000 - 16000 cP
@Shear Rate 230 1/s,
Temperature 77.0 °F
Haake VT 550 PK1.1°
Storage Temperature 20.0 °C68.0 °Fsealed container
 
Processing PropertiesMetricEnglishComments
Cure Time  15.0 min
@Temperature 130 °C
0.250 hour
@Temperature 266 °F
 30.0 min
@Temperature 80.0 °C
0.500 hour
@Temperature 176 °F
Shelf Life 6.00 Month6.00 Month
 
Descriptive Properties
Coverage cm2/g305Using a 230 mesh stainless steel screen with 13 micron emulsion
Material TypeReady-To-Use Formulation
Solvent ResistanceAcetoneAttack
 AcetoneAttack
 DMACAttack
 DMACAttack
 DMFAttack
 DMFAttack
 MEKFull Attack
 MEKFull Attack
 THFAttack
 THFAttack
Solvent SystemEthoxy Propanol or Sericol

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

WGELZ9028 / 139341

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.