MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

LG Chemical LUMIPLAS LD8650I Light diffusion ABS, Injection grade
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), Molded

Material Notes: Light diffusion, Weatherability

Application: (LED) Lamp cover, Signboard, Lighting decoration of electronic device

Information provided by LG Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.20 g/cc0.0434 lb/in³ASTM D792
Linear Mold Shrinkage, Flow 0.0050 - 0.0080 cm/cm
@Thickness 3.20 mm
0.0050 - 0.0080 in/in
@Thickness 0.126 in
ASTM D955
Melt Flow 33 g/10 min
@Load 1.20 kg,
Temperature 300 °C
33 g/10 min
@Load 2.65 lb,
Temperature 572 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 61.8 MPa
@Thickness 3.20 mm
8960 psi
@Thickness 0.126 in
50mm/min; ASTM D638
Elongation at Break >= 100 %
@Thickness 3.20 mm
>= 100 %
@Thickness 0.126 in
50mm/min; ASTM D638
Flexural Strength 93.2 MPa
@Thickness 6.40 mm
13500 psi
@Thickness 0.252 in
15mm/min; ASTM D790
Flexural Modulus 2.26 GPa
@Thickness 6.40 mm
327 ksi
@Thickness 0.252 in
15mm/min; ASTM D790
Izod Impact, Notched 1.47 J/cm
@Thickness 3.20 mm
2.76 ft-lb/in
@Thickness 0.126 in
ASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 126 °C
@Thickness 6.40 mm
259 °F
@Thickness 0.252 in
Unannealed; ASTM D648
UL RTI, Electrical 120 °C248 °FUL 746B
UL RTI, Mechanical with Impact 105 °C221 °FUL 746B
UL RTI, Mechanical without Impact 120 °C248 °FUL 746B
Flammability, UL94  V-2
@Thickness 0.500 mm
V-2
@Thickness 0.0197 in
 V-2
@Thickness 1.60 mm
V-2
@Thickness 0.0630 in
 V-2
@Thickness 2.50 mm
V-2
@Thickness 0.0984 in
 V-2
@Thickness 3.00 mm
V-2
@Thickness 0.118 in
 
Optical PropertiesMetricEnglishComments
Transmission, Visible 65 %
@Thickness 1.00 mm
65 %
@Thickness 0.0394 in
JIS K7361
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 250 - 270 °C482 - 518 °F
Middle Barrel Temperature 260 - 280 °C500 - 536 °F
Front Barrel Temperature 270 - 290 °C518 - 554 °F
Nozzle Temperature 270 - 290 °C518 - 554 °F
Melt Temperature 280 - 300 °C536 - 572 °F
Mold Temperature 60.0 - 100 °C140 - 212 °F
Drying Temperature 100 - 120 °C
@Time 10800 - 18000 sec
212 - 248 °F
@Time 3.00 - 5.00 hour
Moisture Content <= 0.020 %<= 0.020 %
Back Pressure 0.981 - 3.92 MPa142 - 569 psi
Screw Speed 40 - 70 rpm40 - 70 rpm
 
Descriptive Properties
Outdoor Suitabilityf1UL746C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PLHCHEM9804 / 239320

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.