MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Plenco Valite 4224 Novolac Phenolic, Granular, Transfer Molded  (discontinued **)
Categories: Polymer; Thermoset; Phenolic

Material Notes: This Valite product has been replaced by Plenco 4224. Data provided by Plenco.

VALITE 4224 is a brown, two stage, general purpose phenolic molding compound. It has good electrical and moldability characteristics. It is used in electrical and automotive applications and can be molded by compression, transfer, or injection processes. Plenco drop ball 113g test value is 35 cm.


Plenco has discontinued their Valite product line.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.41 g/ccASTM D792
Apparent Bulk Density 0.600 g/ccASTM D1895
Water Absorption 0.35 %ASTM D570
Linear Mold Shrinkage 0.0066 cm/cmPost shrinkage is 0.25% at 72hr 120°C.; ASTM D955
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell E 91ASTM D785
Tensile Strength, Ultimate 53.3 MPaASTM D638
Elongation at Break 0.70 %ASTM D638
Tensile Modulus 8.60 GPaASTM D638
Flexural Yield Strength 81.8 MPaASTM D790
Flexural Modulus 7.80 GPaASTM D790
Compressive Yield Strength 217.9 MPaASTM D695
Izod Impact, Notched 0.200 J/cmASTM D256
Charpy Impact, Notched 0.200 J/cm²J/cm; ASTM D256
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 3.0725e+11 ohm-cmASTM D257
Dielectric Constant 4.9
@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 11.5 kV/mmShort Term per ASTM D149.
Dissipation Factor 0.049
@Frequency 1e+6 Hz
ASTM D150
Arc Resistance 140 secASTM D495
Comparative Tracking Index 175 VASTM D3638
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 193 °CHeat Resistance; ASTM D795
Deflection Temperature at 1.8 MPa (264 psi) 183 °CASTM D648
Flammability, UL94 V-0
@Thickness 6.10 mm

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PLEO81 / 50785

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.