MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Wacker Powersil® PASTE AP Silicone Paste
Categories: Polymer; Thermoset; Silicone

Material Notes: Opaque to whitish paste of medium consistency, good values for electrical insulation, dielectric constant and dielectric strength. POWERSIL® PASTE AP does virtually not show swelling of silicone elastomers that it is in contact with, due to the use of a special, phenylsilicone oil.

Special features:

  • no swelling of bordering silicone elastomers
  • non-curing, with retention of pasty consistency
  • water resistant, water repellent
  • good electrical insulating properties
  • good surface slip
  • high dielectric strength
Application:
  • cable joints
  • cable terminations
  • plugs and connectors
  • sealant and lubricant

Information provided by Wacker Chemie AG.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.10 g/ccISO 1183-1 A
Volatiles <= 5.0 %
@Temperature 200 °C,
Time 108000 sec
FED-STD 791 M 321
 
Mechanical PropertiesOriginal ValueComments
Penetration 250 - 2801/10 mm, unworked; ISO 2137
Penetration P(60), 1/10 mm 280worked; DIN ISO 2137
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 3.7
@Frequency 50 Hz
IEC 60250
Dielectric Strength 20.0 kV/mmDIN 53481
Dissipation Factor 0.00030
@Frequency 50 Hz
IEC 60250
 
Thermal PropertiesOriginal ValueComments
Solidus -45.0 °C
Maximum Service Temperature, Air 200 °C
Minimum Service Temperature, Air -40.0 °C
 
Descriptive Properties
Coloropaque to whitish

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Wacker Wacker® P Silicone Paste
Mitsubishi Iupital® FS2022 Copolymer Acetal
ITW Devcon® Liquid Release Agent Silicone
Evonik TEGOPREN® 5863 Defoamer
Evonik TEGO® Antifoam 3062 Antifoam concentrate

PWACK9395 / 204924

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.