LDF200GG is a low density polyethylene resin for film extrusion. LDF200GG has medium slip and anti-block additives. LDF200GG meets the U.S. Food and Drug Administration (FDA) criteria for food contact use as specified in 21 CFR 177.1520 (c) 2.1 & (c) 2.2. Applications: - Produce bags
- T-shirt carrier bags
- Display packaging
- Light duty shrink film
Additives: Advantages: - Good optical
- Good mechanical properties
Information provided by Titan Chemicals |