MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

MarkeTech Sodium Iodide:Thallium (Nal:Tl) Scintillator Crystal  (discontinued **)
Categories: Ceramic; Halide

Material Notes: Sodium iodide activated by thallium has long been the scintillation standard. Nal:Tl has good performance, economical price, high luminescence efficiency, very good spectroscopic performance and no significant self absorption of the scintillated light.

Data provided by MarkeTech International. MarkeTech International is no longer in business.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 3.67 g/cc0.133 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Mohs 2.02.0
 
Thermal PropertiesMetricEnglishComments
CTE, linear 47.5 µm/m-°C26.4 µin/in-°F
Melting Point 651 °C1200 °F
 
Descriptive Properties
Crystal StructureCubic
Hydroscopic?Yes
Luminescence: Afterglow0.5-5 %at 6 ms
Luminescence: Decay Constant230 n/s
Luminescence: Photon Yield38300K; 103 pH/MeV
Luminescence: Radiation Length2.9 cm
Luminescence: Wavelength of max emissions415 nm

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Sodium Iodide, NaI
Sodium Chloride, NaCl (Halite)
Overview of materials for Polypropylene, Molded
Indium Corp. IndiSul™ In2(SO4)3 - 9H2O Indium Sulfate Hydrated Salt
MarkeTech Sapphire (Aluminum Oxide - Al2O3) Single Crystal

C5MT832 / 120741

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.