MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Dow ELITE™ 5110G Enhanced Polyethylene Resin
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE)

Material Notes: ELITE™ 5110G is a copolymer produced via INSITE™ Technology from Dow Plastics. It offers a unique combination of high modulus and excellent impact strength, allowing for down gauging in bag applications. ELLITE™ 5110G resin complies with U.S. FDA regulation 21 CFR 177.1520 (c) 3.2a when used unmodified and processed according to good manufacturing practices.

Information provided by Dow

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.9255 g/ccASTM D792
Thickness 2.00 mil
Melt Flow 0.85 g/10 minASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Film Tensile Strength at Yield, MD 2015 psiASTM D882
Film Tensile Strength at Yield, TD 2115 psiASTM D882
Film Elongation at Break, MD 597 %ASTM D882
Film Elongation at Break, TD 660 %ASTM D882
Secant Modulus, MD 0.2769 GPa2% Secant; ASTM D882
Secant Modulus, TD 0.3303 GPa2% Secant; ASTM D882
Impact 21.8[lbf]; Puncture Resistance Force; Dow Method
Puncture Energy 61.2 in-lbDow Method
Elmendorf Tear Strength MD 564 gASTM D1922
Elmendorf Tear Strength TD 1110 gASTM D1922
Elmendorf Tear Strength, MD 282 g/milASTM D1922
Elmendorf Tear Strength, TD 555 g/milASTM D1922
Dart Drop Test 409 gMethod B; ASTM D1709
Film Tensile Strength at Break, MD 8339 psiASTM D882
Film Tensile Strength at Break, TD 7534 psiASTM D882
Heat Seal Strength Initiation Temperature 120 °C2 lb/in heat seal strength; 0.5 sec dwell, 40 psi bar pressure, pull speed 10 (in./min.); Dow Method
 
Thermal PropertiesOriginal ValueComments
Melting Point 123 °CDow Method (DSC)
Vicat Softening Point 111 °CASTM D1525
 
Optical PropertiesOriginal ValueComments
Haze 13 %ASTM D1003
Gloss 60 %45°; ASTM D2457
 
Compliance PropertiesOriginal ValueComments
FDA YesSee notes for details.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Dow ELITE™ 5400G Enhanced Polyethylene Resin
Dow ELITE™ 5100G Enhanced Polyethylene Resin
Dow DOWLEX™ 2045G Linear Low Density Polyethylene
Dow ELITE™ 5500G Enhanced Polyethylene Resin
Borealis Borstar® FB2230 LLDPE for Film

PDOW1323 / 30541

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.