MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Ampco Metal AMPCO® 674 Manganese Bronze
Categories: Metal; Nonferrous Metal; Copper Alloy; Bronze

Material Notes: Ampco 673 and 674 are wrought zinc-manganese-silicon lead-copper alloys. Both alloys have excellent capacity for hot forming, with hot forgeability ratings of 100. Ampco 674 exhibits a machinability rating of 25%, while Ampco 673 has a considerably higher rating of 80%. This significant difference in the two materials is in the higher lead content of Ampco 673 which increases that alloy's machinability but decreases its tensile and yield values.

Applications: Widely specified for a variety of bearing and/or corrosive applications: bushings; gears; cams; nuts and bolts; connector rods; idler shafts and other shafting; worm gears; feed fingers; lead nut screws, etc.

Key Words: UNS C67400
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 8.08 g/cc
Density 8.08 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 1833000 kg
Tensile Strength, Ultimate 620 MPa
Tensile Strength, Yield 400 MPa
Elongation at Break 12 %
Modulus of Elasticity 110 GPa
Modulus of Rigidity 41.0 GPa
Poissons Ratio 0.34Calculated
 
Thermal PropertiesOriginal ValueComments
CTE, linear 19.8 µm/m-°C
@Temperature 20.0 °C
Specific Heat Capacity 0.380 J/g-°C
Thermal Conductivity 100 W/m-K
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al 1.6 %
Copper, Cu 57.5 %
Lead, Pb 0.40 %
Manganese, Mn 2.5 %
Silicon, Si 0.70 %
Zinc, Zn 37 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Copper, UNS C67400
High-Leaded Tin Bronze, UNS C93200, Copper Casting Alloy, Bearing Bronze SAE 660
Phosphor bronze 8% Sn, UNS C52100, H02 Temper rod
Aluminum Bronze, UNS C95400, Copper Casting Alloy, As Cast
Ampco Metal AMPCO® 673 Manganese Bronze

NAMPCO36 / 14990

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.