MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Chemours Tefzel® 2195 Fluoropolymer Resin
Categories: Polymer; Thermoplastic; Fluoropolymer; ETFE/ECTFE

Material Notes: DuPont™ Tefzel ® 2195 fluoropolymer is a premium-grade resin designed for use in rotational molding. To be effective as a rotational molding resin, Tefzel ® 2195 is a free-flowing powder, with controlled particle size, shape, and size distribution. The properties of Tefzel ® 2195 in molded form are similar to other grades of Tefzel ® fluoropolymer resin. Table 1 shows typical property data for Tefzel ® 2195.

Rotational molding is a favored process for making hollow parts (particularly large parts) or for parts with complex geometries. Depending on part design and processing conditions, Tefzel ® 2195 can also be used to rotoline items, whereby the Tefzel® binds to the inner surface of the part to form a lining. Properly processed rotational moldings made from Tefzel ® 2195 provide the superior properties typical of the fluoropolymer resins: retention of properties after service at 150°C (302°F), useful properties at –100°C (–148°F), and chemical inertness to most industrial chemicals and solvents. Molded products have excellent stiffness and high ultimate elongation.

Statements, or data, regarding behavior in a flame situation are not intended to reflect hazards presented by this or any other material when under actual fire conditions.

Applications

Tefzel ® 2195 is ideal for many end products for fluid handling in the chemical processing industries, including pump housings, vessels, columns, elbows, tees, and pipe sections with unusual shapes. In addition, any hollow structure with internal contours that permits uniform coating by powder flow is a candidate for lining, provided it can withstand high temperatures.

Chemours was formed from former DuPont performance chemicals businesses, including DuPont Fluoroproducts, in 2015.

Key Words: Ethylene Tetrafluoroethylene Copolymer
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.72 g/ccASTM D792
Bulk Density 0.750 g/cc
Water Absorption <= 0.030 %24 hours; ASTM D570
Particle Size 270 µm
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 72ASTM D2240
Tensile Strength, Ultimate 40.0 - 46.0 MPaASTM D1457
Elongation at Break 150 - 300 %ASTM D1457
Flexural Modulus 1.172 GPaASTM D790
Izod Impact, Notched NBASTM D256
Coefficient of Friction 0.30 - 0.40ASTM D1894
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+17 ohm-cmASTM D257
Surface Resistivity per Square >= 1.00e+15 ohmASTM D257
Dielectric Constant 2.6
@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 79.0 kV/mm100 micrometers film; ASTM D149
Dissipation Factor 0.0070
@Frequency 1e+6 Hz
ASTM D150
Arc Resistance 122 secASTM D495
 
Thermal PropertiesOriginal ValueComments
CTE, linear 90.0 µm/m-°C
@Temperature 0.000 - 100 °C
ASTM D696
Melting Point 253 °CASTM D3418
Maximum Service Temperature, Air 150 °C
Flammability, UL94 V-0
Oxygen Index 30 - 36 %ASTM D2863
 
Processing PropertiesOriginal ValueComments
Processing Temperature 302 - 323 °CCure Temperature
 
Descriptive Properties
20% Hydrochloric Acid Transmission, g/100sq in.<0.02
50% Sodium Hydroxide Transmission, g/100sq in.<.02
Acetic Acid Transmission, g/100sq in.0.41
Acetone Transmission, g/100sq in.0.95
Acetophenone Transmission, g/100sq in.0.5
Benzene Transmission, g/100sq in.0.64
Carbon Tetrachloride Transmission, g/100sq in.0.31
Chemical/Solvent ResistanceExcellent
Ethyl Acetate Transmission, g/100sq in.0.76
Folding Endurance, # cycles, .18-.20 mm10-27 E3
Heat of Combustion J/g13700ASTM D240
Hexane Transmission, g/100sq in.0.56
Piperidine Transmission, g/100sq in.0.04
Red Fuming Nitric Acid Transmission, g/100sq in.7.5-1.4
Salt Spray Resistance on aluminum, Hours1000
Sulfuric Acid Transmission, g/100sq in.0.00001
Water Transmission, g/100sq in.0.4
Weather Resistance15Years unaffected in Florida Exposure

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Chemours Tefzel® 750 Fluoropolymer Resin
Chemours Tefzel® 280 Resin Modified ETFE
Chemours Tefzel® 200 Resin Modified ETFE
Chemours Tefzel® 210 Resin Modified ETFE
Chemours Tefzel® 207 Resin Modified ETFE

PDU9292 / 33359

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.