MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

ExxonMobil Febis K Series 100
Categories: Fluid; Lubricant

Material Notes: Exxon Febis K Series oils are premium quality lubricants designed to satisfy the strictest requirements of machine tool slideways. Their multi-functional performance makes them suitable for combined systems requiring hydraulic, gear and slideway lubrication. They are formulated from high quality mineral base oils and a unique advanced additive package that provides special low frictional characteristics, high oxidation resistance, excellent corrosion protection, outstanding load-carrying performance and special adhesive characteristics to resist wash-off from slideway surfaces. They also exhibit good corrosion prevention for steels and copper alloys completing their all around performance.

Machine tools which provide lubricant to hydraulic systems and slideways from a common system; Machine tools where hydraulic and slideway lubrication systems are separate but the potential for cross-contamination exists; In machinery where steel and copper alloys require lubricant compatibility and corrosion protection; Machine tools where good load-carrying characteristics are desired such as in gears and bearings

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Viscosity Measurement >= 90>= 90Index; ASTM D2270
Kinematic Viscosity at 40°C (104°F) 103.8 cSt103.8 cStASTM D445
 
Thermal PropertiesMetricEnglishComments
Pour Point <= -6.00 °C<= 21.2 °FASTM D97
Flash Point 270 °C518 °FASTM D92
 
Descriptive Properties
Copper Strip Corrosion1B3 hrs @ 100°C
Rust Prevention, Distilled WaterpassASTM D665A

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Chemours Tefzel® 210 Resin Modified ETFE

WEXXON269 / 75694

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.