MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Sandvik Ti3Al2.5V Titanium Tubing
Categories: Metal; Nonferrous Metal; Titanium Alloy

Material Notes: Ti3Al-2.5V tubing offers excellent corrosion resistance to seawater and higher mechanical properties than stainless steels. The Ti-3-2.5 alloy, also known as ASTM Grade 9, is characterized by:
  • Excellent resistance to general corrosion in seawater applications
  • High mechanical strength, superior strength to weight ratio
  • Resistant to stress corrosion cracking in chloride and sour gas environments
  • Excellent resistance to pitting, crevice and erosion corrosion
  • Good formability and weldability
  • Very low thermal expansion
  • Excellent fatigue properties from Sandvik's proprietary processing that controls crystal texture
  • Information provided by Sandvik

    ASTM Grade 9

    Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Physical PropertiesOriginal ValueComments
    Density 4.51 g/cc
     
    Mechanical PropertiesOriginal ValueComments
    Tensile Strength, Ultimate 621 MPaannealed
     862 MPaCWSR
     545 MPa
    @Temperature 800 °C
     860 MPa
    @Temperature 200 °C
    Tensile Strength, Yield 485 MPaannealed
     724 MPaCWSR
    Elongation at Break 10 %CWSR; in 2"
     15 %annealed; in 2"
    Modulus of Elasticity 100 GPaCWSR
     103 GPaannealed
    Charpy Impact 86.0 J
    @Temperature 0.000 °C
     
    Thermal PropertiesOriginal ValueComments
    CTE, linear 9.00 µm/m-°C
    @Temperature 20.0 - 100 °C
    Thermal Conductivity 7.60 W/m-K
    @Temperature 20.0 °C
     9.20 W/m-K
    @Temperature 204 °C
     10.6 W/m-K
    @Temperature 316 °C
     
    Component Elements PropertiesOriginal ValueComments
    Aluminum, Al 2.5 - 3.5 %
    Carbon, C <= 0.10 %
    Hydrogen, H <= 0.013 %
    Iron, Fe <= 0.25 %
    Nitrogen, N <= 0.20 %
    Oxygen, O <= 0.12 %
    Titanium, Ti 92.8 - 95.5 %As balance
    Vanadium, V 2.0 - 3.0 %

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

    Users viewing this material also viewed the following:
    Haynes Hastelloy® B-3® alloy, 0% cold work
    Haynes Ti-3Al-2.5V Alloy Titanium Tubing
    AISI Type S45500 Stainless Steel, hardened at 480°C (900°F) for 4 hours, air cooled
    AISI Type S45500 Stainless Steel, annealed at 815°C (1500°F) for 30 minutes, water quenched, bar
    Sandvik Ti Grade 9 Tube and pipe, seamless

    NSANDV288 / 19182

    Free Trade Publications, Click Here!
    Free Trade Publications, Click Here!

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.