MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Kolon CE700 Polarizing Plate Film  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Polyester, TP

Material Notes: Films for polarizer - defect free polyester base. Films used for protective and adhesive coating during the process of manufacturing polarizer which are used in LCD TVs and Monitors.

Corona treatment possible. Used as release film for polarizer.

Information provided by Kolon

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Film Elongation at Break, MD  170 %
@Thickness 0.0250 mm
170 %
@Thickness 0.000984 in
ASTM D882
 170 %
@Thickness 0.0380 mm
170 %
@Thickness 0.00150 in
ASTM D882
Film Elongation at Break, TD  135 %
@Thickness 0.0250 mm
135 %
@Thickness 0.000984 in
ASTM D882
 135 %
@Thickness 0.0380 mm
135 %
@Thickness 0.00150 in
ASTM D882
Coefficient of Friction, Dynamic  0.40
@Thickness 0.0250 mm
0.40
@Thickness 0.000984 in
ASTM D1894
 0.40
@Thickness 0.0380 mm
0.40
@Thickness 0.00150 in
ASTM D1894
Coefficient of Friction, Static  0.30
@Thickness 0.0380 mm
0.30
@Thickness 0.00150 in
ASTM D1894
 0.35
@Thickness 0.0250 mm
0.35
@Thickness 0.000984 in
ASTM D1894
Film Tensile Strength at Break, MD  245 MPa
@Thickness 0.0250 mm
35500 psi
@Thickness 0.000984 in
ASTM D882
 245 MPa
@Thickness 0.0380 mm
35500 psi
@Thickness 0.00150 in
ASTM D882
Film Tensile Strength at Break, TD  265 MPa
@Thickness 0.0250 mm
38400 psi
@Thickness 0.000984 in
ASTM D882
 265 MPa
@Thickness 0.0380 mm
38400 psi
@Thickness 0.00150 in
ASTM D882
 
Thermal PropertiesMetricEnglishComments
Shrinkage, MD  1.0 %
@Thickness 0.0250 mm
1.0 %
@Thickness 0.000984 in
Heat Shrinkage; ASTM D2305
 1.0 %
@Thickness 0.0380 mm
1.0 %
@Thickness 0.00150 in
Heat Shrinkage; ASTM D2305
Shrinkage, TD  0.00 %
@Thickness 0.0250 mm
0.00 %
@Thickness 0.000984 in
Heat Shrinkage; ASTM D2305
 0.00 %
@Thickness 0.0380 mm
0.00 %
@Thickness 0.00150 in
Heat Shrinkage; ASTM D2305
 
Optical PropertiesMetricEnglishComments
Haze  3.2 %
@Thickness 0.0250 mm
3.2 %
@Thickness 0.000984 in
ASTM D1003
 4.0 %
@Thickness 0.0380 mm
4.0 %
@Thickness 0.00150 in
ASTM D1003
 
Descriptive Properties
Surface Roughness, Ra18 nmJIS B-0601 (Cutoff 0.08)
 18 nmJIS B-0601 (Cutoff 0.08)
Surface Roughness, Rmax800 nmJIS B-0601 (Cutoff 0.08)
 800 nmJIS B-0601 (Cutoff 0.08)

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PKOKZ809 / 185352

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.