Tough, abrasion resistant elastomer Key Properties: - Excellent physical properties after RT cure
- Free of mercury, MOCA or TDI
Applications: - For room temperature hand-batch processing
- For very large parts as well as mass casting.
Cure 1: 24 hours at 77°F + 16 hours at 150°F Cure 2: 7 days at 77°FInformation provided by © RAMPF Tooling Solutions GmbH & Co. KG |