MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Zircar Zirconia ZHB Zirconia Hollow Balls
Categories: Ceramic; Machinable Ceramic; Oxide; Zirconium Oxide

Material Notes: Zirconia Hollow Balls Type ZHB are sintered calcia-stabilized zirconia hollow balls, which flow easily into a confined space. Our standard product is our Type ZHB-1 which ranges in particle size from 0.2 mm to 3.0 mm diameter, which fill space effectively. They are useful for high temperature insulation in spaces where the insulation must be poured into place. The different size balls tend to segregate when poured as the larger balls tend to ‘float’ on top of the smaller balls. To minimize this effect, pour all the balls in at one time.

Application Information:

Zirconia Hollow Balls Type ZHB are useful as heat exchange media in fluidized bed reactors and as insulation in constrained spaces in very high temperature applications. The melting point of ZHB exceeds 4000°F. ZHB can be sieved into a more narrow size distribution on request.

Information provided by Zircar Zirconia.

Key Words: ZrO2, zirconium oxide
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 5.60 g/cc
Bulk Density 1.50 g/cc
 
Component Elements PropertiesOriginal ValueComments
Al2O3 <= 0.80 %
CaO 3.0 - 4.0 %
Fe2O3 <= 0.10 %
HfO2 1.0 - 2.0 %
SiO2 <= 0.60 %
TiO2 <= 0.30 %
ZrO2 >= 91 %
 
Descriptive Properties
Angle of Repose30°
ColorYellow
Crystal Structure80% Cubic, 20% Monoclinic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Magnesia Stabilized Zirconia
Yttria Stabilized Zirconia, YSZ
AISI Type 304L Stainless Steel
AISI Type 304HN Stainless Steel
China-Yixing Longly Refractories ZTA (20%ZrO2) Zirconia Toughened Alumina Composite Ceramic

C6ZIR008 / 2764

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.