MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Westlake Epolene® E-43P Oxidized Low Molecular Weight Polyethylene Polymer
Categories: Polymer; Thermoplastic; Polyethylene (PE)

Material Notes: Description: Epolene E-43P is a maleic anhydride grafted polypropylene powder recommended as a coupling agent for polypropylene (PP) composites and for providing slip resistance in floor finish emulsions. Because of the polarity and anhydride functionality, Epolene E-43P is useful for laminating, as a compatibilizer for PP blends with nylon or EVOH, and for enhancing the strength of composites that utilize reinforcements / fillers such as glass, talc, calcium carbonate, and metals.
    Key Attributes:
  • Coupling agent and compatibilizer for PP composites and alloys
  • Excellent pigment dispersion aid
  • Maleic anhydride grafted polypropylene (PP)
  • Provides slip resistance in floor polish finishes
  • Useful in adhesive blends
    Application/Uses:
  • Automotive
  • Bookbinding
  • Building and Construction
  • Caulks and Sealants
  • Hot Melt Adhesives
  • Laminating
  • Solventborne Adhesives
  • Waterborne Adhesives

Information provided by Westlake Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.920 g/ccASTM D5
Viscosity 100 - 750 cP
@Temperature 190 °C
542-111
Brookfield Viscosity 300 cP
@Temperature 190 °C
Molecular Weight 9100 g/mol
 
Chemical PropertiesOriginal ValueComments
Total Acid Number 45mg KOH/g
 
Thermal PropertiesOriginal ValueComments
Flash Point >= 277 °C
Ring & Ball Softening Point 158 °C
 
Optical PropertiesOriginal ValueComments
Gardner Color Number <= 13542-130
 
Descriptive Properties
Penetration Hardness<1 dmmASTM D5, Needle under 100-g load for 5s @ 25 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Honeywell A-C® 316A High-density oxidized PE homopolymer
Honeywell A-C® 16A Low Density PE homopolymer
Evonik VESTOWAX® A 415 Polyethylene Wax
Westlake Epolene® C-16P Coating Grade - Branched Medium Molecular Weight Polyethylene Polymer
Honeywell A-C® 8 Low Density PE homopolymer

PWESF8909 / 133454

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.