MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

BASF Ultramid® B3W BK102 Nylon 6, Heat Stabilized
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Heat Stabilized

Material Notes: Ultramid B3W BK102 is an unreinforced, heat stabilized, pigmented black, low viscosity, general purpose injection molding PA6 exhibiting excellent fluidity for filling thin sections. It possesses the combination of strength, stiffness and toughness properties as well as excellent chemical, thermal and abrasion resistance. The heat stabilizer system extends its retention of properties at elevated temperatures.

Applications: Ultramid B3W BK102 is generally recommended for applications such as drapery hardware, gears, fittings, furniture casters, bearings, handles, clips and fasteners.

Information provided by BASF.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.13 g/cc0.0408 lb/in³ISO 1183
Water Absorption 1.6 %
@Time 86400 sec
1.6 %
@Time 24.0 hour
ISO 62
Moisture Absorption 2.70 %2.70 %50% RH; ISO 62
Water Absorption at Saturation 9.5 %9.5 %ISO 62
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 36.0 MPa5220 psiConditioned; ISO 527
 85.0 MPa12300 psiDry; ISO 527
Elongation at Break 25 %25 %Dry; ISO 527
 >= 50 %>= 50 %Conditioned; ISO 527
Elongation at Yield 4.0 %4.0 %Dry; ISO 527
 16 %16 %Conditioned; ISO 527
Tensile Modulus 0.970 GPa141 ksiConditioned; ISO 527
 3.10 GPa450 ksiDry; ISO 527
Flexural Strength 25.0 MPa3630 psiConditioned; ISO 178
 90.0 MPa13100 psiDry; ISO 178
Flexural Modulus 0.770 GPa112 ksiConditioned; ISO 178
 2.65 GPa384 ksiDry; ISO 178
Izod Impact, Notched (ISO)  4.00 kJ/m²
@Temperature -40.0 °C
1.90 ft-lb/in²
@Temperature -40.0 °F
Dry; ISO 180
 5.50 kJ/m²
@Temperature 23.0 °C
2.62 ft-lb/in²
@Temperature 73.4 °F
Dry; ISO 180
Charpy Impact Unnotched NBNBDry; ISO 179
Charpy Impact, Notched 0.300 J/cm²1.43 ft-lb/in²Dry; ISO 179
 
Thermal PropertiesMetricEnglishComments
Melting Point 220 °C428 °FISO 3146
Deflection Temperature at 1.8 MPa (264 psi) 60.0 °C140 °FISO 75
 
Processing PropertiesMetricEnglishComments
Melt Temperature 240 - 285 °C464 - 545 °F
Mold Temperature >= 10.0 °C>= 50.0 °Fcan be used where applicable.
 65.0 - 80.0 °C149 - 176 °Frecommended
Drying Temperature 80.0 °C
@Time 7200 - 14400 sec
176 °F
@Time 2.00 - 4.00 hour
Moisture Content <= 0.15 %<= 0.15 %
Injection Pressure 3.45 - 10.3 MPa500 - 1500 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PBASF8965 / 254923

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.