MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Parson Adhesives SONLOCK™ 3242 Anaerobic Thread Locking Compound
Categories: Polymer; Adhesive

Material Notes: SONLOK 3242 is a fast curing, medium strength anaerobic thread locking compound for bonding and sealing threads, and retaining of cylindrical parts. SONLOK 3242 is highly resistance to heat, vibrations, water, gases, oils, hydrocarbons and many chemicals.

Applications:

  • Ideal for thread locking plated parts, vibration or moving components.
  • Ideal for fasteners between ¼” and ¾” (6 to 20 mm) diameters.
  • Locks and seals threaded joints-nuts, screws, and studs.
  • Meets 90% of all nut and bolt thread locking applications.
  • Meets Military specifications: MIL-S-46163 Type II Grade N; MIL-S-22473E Letter Grade CVV

Information provided by Parson Adhesives, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.07 g/cc1.07 g/cc
Brookfield Viscosity 1200 cP1200 cPRVT, Spindle 3 @ 20 rpm
 
Thermal PropertiesMetricEnglishComments
CTE, linear 80.0 µm/m-°C44.4 µin/in-°FASTM D696 K-1
Specific Heat Capacity 0.300 J/g-°C0.0717 BTU/lb-°F
Thermal Conductivity 0.100 W/m-K0.694 BTU-in/hr-ft²-°FASTM C177
Maximum Service Temperature, Air 150 °C302 °F
Minimum Service Temperature, Air -55.0 °C-67.0 °F
Flash Point >= 100 °C>= 212 °F
 
Processing PropertiesMetricEnglishComments
Cure Time 10.0 min0.167 hourHandling
 60.0 - 180 min1.00 - 3.00 hourFunctional
 1440 min24.0 hourFull
Shelf Life 24.0 Month24.0 Month
 
Descriptive Properties
ColorBlue
CompositionMethacrylate Ester
Diameter<0.2 mmThread/Gap Filling
Initial Strength Retained (%)100Ethanol for 500 hrs at 22°C
 100Ethanol for 1000 hrs at 22°C
 100Motor Oil for 500 hrs at 125°C
 100Motor Oil for 1000 hrs at 125°C
 100Gasoline for 500 hrs at 22°C
 100Acetone for 500 hrs at 22°C
 100Break Fluid for 500 hrs at 22°C
 100Break Fluid for 1000 hrs at 22°C
 80Water/Glycol for 1000 hrs at 87°C
 85Acetone for 1000 hrs at 22°C
 90Water/Glycol for 500 hrs at 87°C
 95Gasoline for 1000 hrs at 22°C
Torque1-4 NmPrevail, 3/8x16 zinc nuts and bolts, ISO 10964
 1-5 NmPrevail, 3/8x16 cadmium nuts and bolts, ISO 10964
 1-7 NmBreakaway, 3/8x16 cadmium nuts and bolts, ISO 10964
 2-7 NmBreakaway, 3/8x16 zinc nuts and bolts, ISO 10964
 3-7 NmPrevail, 3/8x16 steel nuts and bolts, ISO 10964
 8-17 NmBreakaway, 3/8x16 steel nuts and bolts, ISO 10964
 8-19 NmBreakaway, M10 black oxide steel nuts and bolts, ISO 10964

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PPARSN015 / 186458

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.