MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Domo TechnylStar™ A205 F Natural S PA6, Eh 0
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Unreinforced

Material Notes: Description: TECHNYLSTAR A205 F NATURAL S is a polyamide 6.6 with low viscosity for fast cycle molding.

Colors: it is supplied in natural color.

Available in: Latin America and North America

Main Properties: High Fluidity, V2 UL 94 Classification and Glow wire Resistance

Applications: This product is indicated for various applications at automotive and electric & electronic industries.

DOMO Chemicals has acquired Solvay’s Performance Polyamides Business in Europe.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.15 g/cc0.0415 lb/in³ISO 1183/A
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 80.0 MPa11600 psiISO 527
Elongation at Break 32 %32 %ISO 527
Tensile Modulus 3.30 GPa479 ksiISO 527
Flexural Modulus 3.07 GPa445 ksiISO 178
Izod Impact, Notched (ISO) 3.50 kJ/m²1.67 ft-lb/in²ISO 180
Charpy Impact Unnotched NBNBISO 179
Charpy Impact, Notched 0.340 J/cm²1.62 ft-lb/in²ISO 179
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+14 ohm-cm1.00e+14 ohm-cmCEI 93
Dielectric Constant 2.92.9CEI 250
Dielectric Strength 27.0 kV/mm686 kV/inCEI 93
Dissipation Factor 0.0300.030CEI 250
Comparative Tracking Index 600 V600 VCEI 112
 
Thermal PropertiesMetricEnglishComments
Melting Point 262 °C504 °FASTM D3418
Deflection Temperature at 1.8 MPa (264 psi) 69.0 °C156 °FISO 75
Flammability, UL94 V-2
@Thickness 1.60 mm
V-2
@Thickness 0.0630 in
Glow Wire Test 960 °C1760 °FCEI 695
 
Processing PropertiesMetricEnglishComments
Feed Temperature 265 - 275 °C509 - 527 °F
Mold Temperature 60.0 - 80.0 °C140 - 176 °F
 
Descriptive Properties
Compression Zone270-285°C
Mixing Zone270-285°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Domo TechnylStar™ A205 F Natural S PA66, Eh 50
Aluminum 2050 Composition Spec
Aluminum 201.0-T6 Casting Alloy
Cast Stainless Steel 17- 4, UNS J92150 (Compostion Spec)
Carpenter Custom 630 (17-Cr-4Ni) Precipitation Hardening Stainless Steel, Annealed

PRHOD817 / 138048

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.