P601F is a homopolymer polypropylene resin for water-quenched blown film resin. This grade is contain high slip and antiblock agent and recommended for applications that film thickness is lower than 50 micron. Applications: Food packaging. Outer packing bag. Shopping bag. Features: High productivity. Good optical properties. Excellent open-ability. Food contact applicable. High slip and ant-block content. Information provided by SCG. |