MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Antimony, Sb
Categories: Metal; Nonferrous Metal; Pure Element

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 6.618 g/cc
 
Chemical PropertiesOriginal ValueComments
Atomic Mass 121.7601995
Atomic Number 51
Thermal Neutron Cross Section 5.7 barns/atom
X-ray Absorption Edge 0.40663 ÅK
 2.63296 ÅLI
 2.82304 ÅLII
 2.99637 ÅLIII
Electrode Potential 0.10 V
Electronegativity 2.05Pauling
Ionic Radius 0.620 ÅCrystal Ionic Radius for Valence +5
 0.760 ÅCrystal Ionic Radius for Valence +3
 2.45 ÅCrystal Ionic Radius for Valence -3
Electrochemical Equivalent 1.494 g/A/h
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 30 - 58
Hardness, Vickers 30 - 60
Tensile Strength, Ultimate 11.4 MPa
Modulus of Elasticity 77.759 GPa
Shear Modulus 19.0 GPa
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000410 ohm-cm
Magnetic Susceptibility -8.13e-7cgs/g
Critical Superconducting Temperature 2.60 - 2.70 K
 3.40 - 3.55 K
@Pressure 8500 - 15000 MPa
Sb III
 
Thermal PropertiesOriginal ValueComments
Heat of Fusion 168.3 J/g
Heat of Vaporization 1604 J/g
CTE, linear 10.9 µm/m-°C
@Temperature 20.0 - 100 °C
Specific Heat Capacity 0.206 J/g-°C
Thermal Conductivity 18.6 W/m-K
Melting Point 630.74 °C
Boiling Point 1587 °C
 
Optical PropertiesOriginal ValueComments
Reflection Coefficient, Visible (0-1) 0.7058.9 micron wavelength
 
Component Elements PropertiesOriginal ValueComments
Antimony, Sb 100 %
 
Descriptive Properties
CAS Number7440-36-0

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Silver, Ag
Bismuth, Bi
Gallium, Ga
Sodium, Na
Cesium, Cs

AMESb00 / 99

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.