MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
AK Steel PH 15-7 Mo® Precipitation Hardening Stainless Steel, Condition CH 900
Categories: Metal; Ferrous Metal; Martensitic; Stainless Steel; Precipitation Hardening Stainless

Material Notes: AK Steel 15-7 Mo® provides high strength and hardness, good corrosion resistance and minimum distortion on heat treatment. It is easily formed in the annealed condition and develops effective balance of properties by simple heat treatment. This alloy is useful for a wide range of applications that include retaining rings, springs, diaphragms, aircraft bulkheads, welded and brazed honeycomb paneling and other aircraft components requiring high strength at elevated temperatures.

The material supplied from the mill is in Condition A. After fabrication, and conditioning treatments, the material is precipitation hardened into either Condition TH 1050 or Condition RH 950. To achieve the highest mechanical properties Condition A material is transformed to martensite at the mill by cold reduction to Condition C. After fabrication by the user a single low-temperature heat treatment is preformed to achieve condition CH 900.

Information provided by AK Steel

Key Words: UNS S15700
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.70 g/ccTypical
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell C 50
Tensile Strength, Ultimate 1828 MPa
Tensile Strength, Yield 1793 MPa
@Strain 0.2 %
Elongation at Break 2.0 %in 2 inches
Modulus of Elasticity 200 GPa
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al 0.75 - 1.5 %
Carbon, C <= 0.090 %
Chromium, Cr 14 - 16 %
Iron, Fe 69.58 - 76.75 %As Remainder
Manganese, Mn <= 1.0 %
Molybdenum, Mo 2.0 - 3.0 %
Nickel, Ni 6.5 - 7.75 %
Phosphorus, P <= 0.040 %
Silicon, Si <= 1.0 %
Sulfur, S <= 0.040 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
AK Steel PH 15-7 Mo® Precipitation Hardening Stainless Steel, Condition RH 950
AK Steel PH 15-7 Mo® Precipitation Hardening Stainless Steel, Condition TH 1050
AK Steel PH 15-7 Mo® Precipitation Hardening Stainless Steel, Condition C
AK Steel PH 15-7 Mo® Precipitation Hardening Stainless Steel, Condition A
AISI Type S14800 Stainless Steel condition CH900, 39.2% cold reduction

NAKS127 / 14730

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.