MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Nouryon Armeen T Tallow amine
Categories: Other Engineering Material

Material Notes: Armeen T is a tallow amine

Information provided by Nouryon

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density  0.791 g/cc
@Temperature 70.0 °C
0.0286 lb/in³
@Temperature 158 °F
 0.799 g/cc
@Temperature 60.0 °C
0.0289 lb/in³
@Temperature 140 °F
 0.814 g/cc
@Temperature 38.0 °C
0.0294 lb/in³
@Temperature 100 °F
Viscosity  37.8 cP
@Temperature 75.0 °C
37.8 cP
@Temperature 167 °F
 38.8 cP
@Temperature 65.0 °C
38.8 cP
@Temperature 149 °F
 40.6 cP
@Temperature 55.0 °C
40.6 cP
@Temperature 131 °F
 44.4 cP
@Temperature 45.0 °C
44.4 cP
@Temperature 113 °F
Vapor Pressure 0.000133322 bar0.0999998 torr
 
Thermal PropertiesMetricEnglishComments
Specific Heat Capacity  2.05 J/g-°C
@Temperature 25.0 - 30.0 °C
0.490 BTU/lb-°F
@Temperature 77.0 - 86.0 °F
 2.18 J/g-°C
@Temperature 37.2 - 42.2 °C
0.520 BTU/lb-°F
@Temperature 99.0 - 108 °F
 2.26 J/g-°C
@Temperature 45.0 - 48.9 °C
0.540 BTU/lb-°F
@Temperature 113 - 120 °F
Melting Point 40.0 °C104 °F
Boiling Point 260 - 350 °C
@Pressure 0.101325 MPa
500 - 662 °F
@Pressure 14.6921 psi
Pour Point 35.0 °C95.0 °F
Flash Point >= 100 °C>= 212 °F
 
Optical PropertiesMetricEnglishComments
Gardner Color Number 0.00 - 3.00.00 - 3.0
 
Component Elements PropertiesMetricEnglishComments
H2O, Water <= 0.50 %<= 0.50 %
 
Descriptive Properties
Amine number209-217 mg KOH/g
AppearanceSolid
Cloud point43°C
Content=5%(Mw=507), Secondary + Tertiary Amine
 =95%(Mw=262), Primary Amine
 40-60 g I2/100 gIodine value
Equivalent mass267 g/eq
HLB8.2Davies Scale 0-40

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PNOURY219 / 285742

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.