Low Odour Series: very low viscosity and low blooming. The Low Odour Series stands for Cyanoacrylates with low odor, low blooming (whitening effect) and low outgasing characteristics. These very positive properties unfortunately go along with lower strength features compared to the Ethylester based Cyanoacrylates. CB 5500 is a very low viscosity grade with wicking properties.Information provided by H.B. Fuller Company |