MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Omni Plastics OmniCarb™ PC/ABS GR10 PC/ABS, 10% Glass Reinforced
Categories: Polymer; Thermoplastic; ABS Polymer; Polycarbonate/ABS Alloy, Glass Fiber Filled

Material Notes: 10% Glass Reinforced; values are based on natural or black materials unless otherwise noted.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.22 g/ccASTM D792
Filler Content 10 %ASTM D2584
Melt Flow 10 g/10 minASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 57.0 MPaASTM D638
Elongation at Break 3.0 %ASTM D638
Flexural Strength 83.0 MPaASTM D790
Flexural Modulus 3103 MPaASTM D790
Izod Impact, Notched 91.0 J/m
@Thickness 3.17 mm
ASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 132 °C
@Thickness 3.17 mm
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 121 °C
@Thickness 3.17 mm
ASTM D648
Flammability, UL94 HB
@Thickness 3.17 mm
Omni Internal Testing
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 480 - 560 °F
Middle Barrel Temperature 520 - 580 °F
Front Barrel Temperature 520 - 580 °F
Nozzle Temperature 520 - 580 °F
Melt Temperature 520 - 580 °F
Mold Temperature 150 - 250 °F
Drying Temperature 250 °F
Dry Time 3.00 - 4.00 hour
Moisture Content <= 0.020 %
Back Pressure 25.0 - 50.0 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Lotte Advanced Materials Infino® LS-1159 PC/ABS/ 15% GF
MRC Polymers NAXALOY™ 770 GF16 ABS+PC Alloy, 16% Glass Fiber Filled
Lotte Advanced Materials Infino® LB-1010W PC, Unreinforced FR
Overview of materials for Polycarbonate/ABS Alloy, Glass Fiber Filled
Daicel CEVIAN® S1220 PC/ABS alloy

POMNI5115 / 185261

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.