MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Dow Prevail® 3100 ABS + Polyurethane
Categories: Polymer; Thermoplastic; ABS Polymer; ABS/Polyurethane Alloy; Polyurethane, TP

Material Notes: PREVAIL® 3100 thermoplastic resin offers designers and manufacturers a combination of flexibility and low temperature toughness not previously available in an engineering thermoplastic and is used for applications ranging from flexible bumper fascias to sports equipment components. It is easy to process and is paintable without the need for a primer.

Data provided by Dow Chemical.

Key Words: Poly(Acrylonitrile Butadiene Styrene)
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.10 g/ccASTM Data
Linear Mold Shrinkage 0.0060 cm/cm
Melt Flow 16 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ASTM Data
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 27.6 MPaASTM Data
Tensile Strength, Yield 26.9 MPaASTM Data
Elongation at Break 200 %ASTM Data
Elongation at Yield 28 %ISO Data
Tensile Modulus 0.496 GPaASTM Data
Izod Impact, Notched NBASTM Data
 7.48 J/cm
@Temperature -50.0 °C
ASTM Data
Charpy Impact Unnotched NBISO Data
 NBISO Data, Low Temp
Charpy Impact, Notched 7.00 J/cm²ISO Data, Low Temp
 10.0 J/cm²ISO Data
Instrumented Impact Total Energy 51.4 J
@Temperature 23.0 °C
 65.5 J
@Temperature -30.0 °C
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 90.0 µm/m-°C
@Temperature 20.0 °C
ASTM data
Deflection Temperature at 0.46 MPa (66 psi) 71.0 °CUnannealed; ASTM Data
 92.0 °CAnnealed; ASTM Data
Deflection Temperature at 1.8 MPa (264 psi) 57.0 °CUnannealed; ASTM Data
 75.0 °CAnnealed; ASTM Data
Vicat Softening Point 101 °C
 
Optical PropertiesOriginal ValueComments
Gloss 76 %Gardner Gloss, 60°

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for ABS/Polyurethane Alloy
Overview of materials for ABS/Polyester Alloy
Dow Prevail® 3150 ABS + Polyurethane
Dow Prevail® 3050 ABS + Polyurethane
Covestro Desmopan® DP 8715 Polyurethane + ABS

PDW120 / 34351

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.