MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Teknor Apex Vital-Line SHM1332B Rigid Polyvinyl Chloride
Categories: Polymer; Thermoplastic; Vinyl (PVC); PVC, Rigid Grade

Material Notes: Availability: Asia Pacific. Form : pellets. Features: ethylene oxide sterilizable, non-phthalate plasticizer, radiation sterilization. Processing Method: injection molding. Uses: medical / healthcare applications.

Typical temperature profile for processing compound is from 145°C to 190°C. The optimum temperatures depend on the type of machine as well as screw design being used to process. Feeding zone: 145°C, barrel zone: 150-165°C, mold temperature: 0°C-50°C, nozzle zone: 165-190°C.

Information provided by Teknor Apex.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.34 - 1.38 g/cc0.0484 - 0.0499 lb/in³ASTM D792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 75 - 8175 - 81ASTMD2240
Tensile Strength, Yield >= 29.4 MPa>= 4270 psi20 in/min; ASTM D638
Elongation at Break >= 10 %>= 10 %ASTM D638
Flexural Modulus >= 2.60 GPa>= 377 ksiASTM D790
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point >= 80.0 °C>= 176 °F1 kg; ASTM D1525
 
Descriptive Properties
Heat Stability> 30 min, ASTM D2115-92, 374°F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
GEHR Plastics PVC-U Polyvinylchloride
Inovyn 260RF Polyvinyl Chloride General Purpose - Rigid
Colorite Polymers 2019F Rigid PVC
BASF Vinidur® Compound DB 8316 white PVC, Unplasticized
Axiall CL-7049 Rigid PVC, Molding

PTEKNN9629 / 231030

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.