MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Cri-Tech FKX-719-75 FKM Fluoroelastomer, Durometer 75A
Categories: Polymer; Thermoset; Fluoropolymer, TS; Thermoset Fluoroelastomer; Rubber or Thermoset Elastomer (TSE)

Material Notes: The LS compounds are designed to give part shrinkage (out of the mold) and post-curing operation comparable to a nitrile or similar elastomers. In most cases, tooling changes are not required when switching over to an LS compound. NPC indicates no post-cure required to achieve high tensile and modulus values with good compression set and aging characteristics. FKHT is a high temperature resistant, low compression set compound. FKX is a high viscosity, high green strength, black fluorocarbon compound formulated for HAV and/or salt bath curing of O-ring cord and extruded profiles.

Information provided by Cri-Tech Performance Materials, an independent subsidiary of Daikin America.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.84 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 75
Tensile Strength 2090 psi
Elongation at Break 190 %
100% Modulus 1100 psi
@Strain 100 %
Compression Set 12 %
@Temperature 200 °C,
Time 79200 sec
Plied disc

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Cri-Tech FDA-615-65-THK FKM Fluoroelastomer, Durometer 66A
Cri-Tech LC-615-65-THK FKM Fluoroelastomer, Durometer 68A
Cri-Tech IF-815 FKM Fluoroelastomer, Durometer 81A
Cri-Tech HFLT-820 FKM Fluoroelastomer, Durometer 82A
Cri-Tech HFLT-720-75 FKM Fluoroelastomer, Durometer 74A

PDAIK908 / 210161

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.