MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Rogers Arlon R36338R015 0.0155" (0.394 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Categories: Polymer; Thermoset; Silicone; Silicone Rubber; Silicone, Molded, Glass Fiber Filled

Material Notes: Design/Construction:
Interleave: Polyethylene
Side 1, Layer 2: Uncured Silicone Rubber
Side 1, Layer 1: Uncured Silicone Rubber
Substrate: Style 7628 Fiberglass
Side 2: Cured Silicone Rubber

Appearance: Red colored, high viscosity gum on fiberglass fabric

This data represents typical values for the production material. The data should not be used to write, or in place of, material specifications.

Information provided by Arlon Silicone Technologies Division; now a part of Rogers Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.17 g/ccSilicone Property; Arlon SQA-TMS-024
Thickness 0.750 milSide 1, Cured; Arlon SQA-TMS-003
 0.750 milSide 2; Arlon SQA-TMS-003
 1.50 milInterleave
 6.00 milSide 1, Uncured; Arlon SQA-TMS-003
 8.00 milSubstrate; Arlon SQA-TMS-003
 15.5 milOverall; Arlon SQA-TMS-003
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 23Silicone Property; ASTM D2240
Tensile Strength 650 psiSilicone Property; ASTM D412
Elongation at Break 1150 %Silicone Property; ASTM D412
Peel Strength 10.0 pliBond Strength (S1 to S2); ASTM D624
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength 775 V/milASTM D149
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 450 °F
Minimum Service Temperature, Air -70.0 °F
 
Processing PropertiesOriginal ValueComments
Cure Time 2.00 hour
@Temperature 204 °C
Recommended Postcure Cycle
 15.0 min
@Pressure 0.345 - 0.517 MPa,
Temperature 110 °C
Recommended Cure Cycle
Shelf Life 6.00 Month
@Temperature 4.44 - 10.0 °C
From date of manufacture
 
Descriptive Properties
ColorRed
Total Product Weight (oz/yd2)16.5Arlon SQA-TMS-025

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Elkem (Bluestar Silicones) BLUESIL™ V-330 CA-35 Silicone Rubber
Teknor Apex Monprene® MP-2287M Thermoplastic Elastomer
Silikony Polskie Gumosil K Silicone Rubber
Polynorbornene Rubber (PNR)
Momentive Performance Materials Silopren™ LSR 2020 Liquid Silicone Rubber - General Purpose

PARL647 / 125833

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.