MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Lubriplate Shield Gear Lithium Based Grease For Open Gearing
Categories: Fluid; Lubricant; Lithium Gellant

Material Notes: Lithium-based open gear grease made for all types of open gears. Available in 4 formulas for a variety of conditions and temperatures.

Applications: Open gears, normal conditions.

Gear Shield Series Greases are available in Cans, Pails, 1/4 Drums & Drums.

Information provided by Lubriplate

Key Words: Part Number L0150-
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Saybolt Viscosity at 100°F 1250 SUS1250 SUS
Kinematic Viscosity at 40°C (104°F) 237 cSt237 cSt
 
Mechanical PropertiesMetricEnglishComments
Penetration P(0), 1/10 mm 310310Unknown Amount of Work
Penetration P(60), 1/10 mm 340340Unknown Amount of Work
 
Thermal PropertiesMetricEnglishComments
Minimum Service Temperature, Air -28.9 °C-20.0 °FApprox. Cold test
Dropping Point 177 °C350 °FASTM Test
 
Descriptive Properties
Antiwear (AW)/ Extreme Pressure (EP)AW
NLGI Grade1
Rust/Oxidative AdditivesYES
Water ResistantYES

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

WLUBR080 / 76126

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.