MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Saint-Gobain CHR® 2285-5 Extruded PTFE Film Backing Silicone Adhesive Pressure Sensitive Tape
Categories: Polymer; Adhesive; Tape; Thermoset; Silicone

Material Notes: CHR® 2283 and 2285 are manufactured from extruded, oriented, high-modulus PTFE film coated with high-temperature pressuresensitive adhesive.

Features/Benefits: The high-temperature resistance and anti-stick properties of PTFE make CHR® 2283 and 2285 ideal products to be used as a release surface. Extremely durable and abrasion resistant, they will not curl or wrinkle making it long-wearing and easy to apply. They will not leave an adhesive residue when removed, resulting in less equipment down time.

Applications: CHR® 2283 and 2285 are ideal tapes for protecting extrusion and laminating equipment during the plastic extrusion coating process which combines plastic films with various substrates, most commonly paper. During this process, plastics are extruded onto the substrate as it passes between a neoprene roller and a cooling roller. Saint-Gobain Performance Plastics 2283 and 2285 are used as a roller wrapping tape to protect the exposed ends of the neoprene roller from the molten plastic which is over-coated wider than the substrate.
Information provided by Saint Gobain Performance Products.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Elongation at Break 200 %
Tear Strength 75.0 pliInitial Tear Strength
Peel Strength 0.440 kN/mAdhesion to Steel
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength 2460 V/mil
Dielectric Breakdown 16000 V
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 500 °F
Minimum Service Temperature, Air -100 °F
 
Descriptive Properties
ColorRust

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSTGQZ366 / 68880

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.