MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Covestro Arcol® HS-200 Polyol
Categories: Polymer; Thermoset

Material Notes: Characterization: Arcol HS-200 polyol is a premium high-load polymer polyol with the highest polymer solids content of commercial polyols.

Properties / Applications Arcol HS-200 polyol is used in the manufacture of high load flexible foams. It is designed to provide the highest polymer content at the lowest viscosity. It also helps to control the rise time to give greater process latitude and the potential for improved foam yield and reduced scrap. As with any product, use of HS-200 in a given application must be tested (including but not limited to field testing) in advance by the user to determine suitability.

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.06 g/cc1.06 g/cc
Bulk Density 1.08 g/cc0.0389 lb/in³
Solids Content 49 %49 %
Viscosity 4210 cP4210 cP
 2500 cP
@Temperature 38.0 °C
2500 cP
@Temperature 100 °F
 5000 cP
@Temperature 23.0 °C
5000 cP
@Temperature 73.4 °F
 10000 cP
@Temperature 12.0 °C
10000 cP
@Temperature 53.6 °F
 15000 cP
@Temperature 9.00 °C
15000 cP
@Temperature 48.2 °F
Storage Temperature 20.0 - 60.0 °C68.0 - 140 °F
 
Thermal PropertiesMetricEnglishComments
Flash Point 213 - 232 °C415 - 450 °FPMCC
 
Processing PropertiesMetricEnglishComments
Moisture Content <= 0.060 %<= 0.060 %
 
Descriptive Properties
AppearanceWhite, viscous liquid
Hydroxyl number23.5-27.5 mg KOH/g

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Covestro Arcol® F-1080 Polyol
Covestro Arcol® F-3040 Polyol
Covestro Arcol® F-3022 Polyol
Covestro Arcol® F-1522 Polyether Polyol
Covestro Arcol® E-919 Polyether Polyol

PCOVEST0026 / 201809

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.