MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
EMS-Grivory Grilon® BG-25 S PA6-GF25
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 30% Glass Fiber Filled

Material Notes: Product description: Grilon BG-25 S is a heat stabilized PA6 injection molding grade with 25 % glass fibers. Grilon BG-25 S has the following important properties:
  • Excellent surface finish
  • Easy flowing
  • Easy processing
Application examples are automotive applications such as handles and levers and fixing parts in the electronic field.

Information provided by EMS Grivory.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.31 g/ccDry; ISO 1183
Water Absorption 7.0 %Sim. to ISO 62
Moisture Absorption 2.00 %Sim. to ISO 62
Linear Mold Shrinkage, Flow 0.0010 cm/cmISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.0050 cm/cmISO 294-4, 2577
 
Mechanical PropertiesOriginal ValueComments
Ball Indentation Hardness 90.0 MPaConditioned; ISO 2039-1
 185 MPaDry; ISO 2039-1
Tensile Strength at Break 90.0 MPaConditioned; ISO 527-1/-2
 165 MPaDry; ISO 527-1/-2
Elongation at Break 3.0 %Dry; ISO 527-1/-2
 8.0 %Conditioned; ISO 527-1/-2
Tensile Modulus 4800 MPaConditioned; ISO 527-1/-2
 8500 MPaDry; ISO 527-1/-2
Charpy Impact Unnotched 70.0 kJ/m²
@Temperature -30.0 °C
Dry; ISO 179/1eU
 70.0 kJ/m²
@Temperature -30.0 °C
Conditioned; ISO 179/1eU
 85.0 kJ/m²
@Temperature 23.0 °C
Dry; ISO 179/1eU
 85.0 kJ/m²
@Temperature 23.0 °C
Conditioned; ISO 179/1eU
Charpy Impact, Notched 9.00 kJ/m²
@Temperature -30.0 °C
Dry; ISO 179/1eA
 9.00 kJ/m²
@Temperature -30.0 °C
Conditioned; ISO 179/1eA
 10.0 kJ/m²
@Temperature 23.0 °C
Dry; ISO 179/1eA
 20.0 kJ/m²
@Temperature 23.0 °C
Conditioned; ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+10 ohm-cmConditioned; IEC 60093
 1.00e+12 ohm-cmDry; IEC 60093
Surface Resistance 1.00e+11 ohmIEC 60093
Dielectric Strength 29.0 kV/mmConditioned; IEC 60243-1
 30.0 kV/mmDry; IEC 60243-1
Comparative Tracking Index 575 VConditioned; IEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 25.0 µm/m-°CISO 11359-1/-2
CTE, linear, Transverse to Flow 80.0 µm/m-°CISO 11359-1/-2
Melting Point 222 °C10°C/min; ISO 11357-1/-3
Maximum Service Temperature, Air 90.0 - 110 °CLong Term; ISO 2578
 160 °CShort Term; EMS
Deflection Temperature at 1.8 MPa (264 psi) 205 °CISO 75-1/-2
Deflection Temperature at 8.0 MPa 125 °CISO 75-1/-2
Flammability, UL94 HBIEC 60695-11-10
 
Descriptive Properties
AutomotiveAir intake systems
 Interior
Electricals & ElectronicsElectrical appliances
 Electrical equipment
FormGranules
ProcessingInjection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
EMS-Grivory Grilon® EBV-2H PA6-GF20
EMS-Grivory Grilon® BG-25 HM PA6-GF25
Celanese Zytel® 73G30L NC010 PA6-GF30
BASF Ultramid® B3WG5 25% Glass Filled PA6 (Dry)
LG Chemical LUMID GP2251AF PA6+GF25%, Flame Retardant

PGRH168 / 156877

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.